Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 72ni 15.5cr 0.95(Cb + Ta) 2.5ti 0.70al 7.0fe, Equalized, Precipitation Hardenable AMS5667K

This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging, flash welded rings, or heading.

These products have been used typically for parts, such as bolts and turbine rotors, requiring high strength in the range of 800 to 1100 degrees F (427 to 593 degrees C), but usage is not limited to such applications.

AMS5667N
2015-01-07
Latest
Revised
AMS5667M
2008-08-28
Historical
Revised
AMS5667L
2003-06-03
Historical
Revised
AMS5667K
1996-05-01
Historical
Revised
AMS5667J
1990-04-01
Historical
Revised
AMS5667H
1979-07-01
Historical
Revised
AMS5667G
1972-05-01
Historical
Revised
AMS5667F
1960-01-01
Historical
Revised
AMS5667E
1958-08-01
Historical
Revised
AMS5667D
1953-12-01
Historical
Revised
AMS5667C
1951-06-01
Historical
Revised
AMS5667B
1950-06-01
Historical
Revised
AMS5667A
1949-03-01
Historical
Revised
AMS5667
1947-12-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 18% off list price.
Login to see discount.
Special Offer: Purchase more aerospace standards and aerospace material specifications and save! AeroPaks offer a customized subscription plan that lets you pay for just the documents that you need, when you need them.

Get Involved

Want to participate in updating this standard?

X