Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 °F (954 °C) Solution, Stabilization, and Precipitation Heat Treated AMS5703E

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, flash welded rings up to 4.00 inch, incl (101.6 mm, incl) in nominal diameter or least distance between parallel sides, and stock of any size for forging or flash welded rings (see 8.5).
AMS5703F
2023-08-22
Latest
Revised
AMS5703E
2018-03-04
Historical
Revised
AMS5703D
2012-02-09
Historical
Reaffirmed
AMS5703C
2000-09-01
Historical
Reaffirmed
AMS5703B
1988-01-01
Historical
Revised
AMS5703A
1981-07-01
Historical
Revised
AMS5703
1971-11-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable

AMS5747E

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1750 °F (954 °C) Solution Heat Treated

AMS5702E

View Details

STANDARD

Nickel - Copper Alloy, Corrosion-Resistant, Bars and Forgings 67Ni - 30Cu - 0.04S Free Machining

AMS4674H

View Details

Get Involved

Want to participate in updating this standard?

X