Browse Standards AMS5704K
Current REVISED 2015-01-14

Nickel Alloy, Corrosion and Heat-Resistant, Forgings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated AMS5704K

This specification covers a corrosion and heat-resistant nickel alloy in the form of forgings 3.25 inches (82.6 mm) and under, and forging stock of any size. (See 8.5).
AMS5704K
2015-01-14
Latest
Revised
AMS5704J
2013-12-02
Historical
Reaffirmed
AMS5704H
2006-05-17
Historical
Revised
AMS5704G
2000-10-01
Historical
Revised
AMS5704F
1995-04-01
Historical
Revised
AMS5704E
1993-10-01
Historical
Revised
AMS5704D
1988-04-01
Historical
Revised
AMS5704C
1982-01-01
Historical
Revised
AMS5704B
1976-01-01
Historical
Revised
AMS5704A
1970-05-01
Historical
Revised
AMS5704
1966-03-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.

Due to current capacity constraints, printed versions of our publications - including standards, technical papers, EDGE Reports, scholarly journal articles, books, and paint chips - may experience shipping delays of up to four to six weeks. We apologize for any inconvenience.
We also recommend:
STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated

AMS5707N

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings Ni - 18Cr - 2.8Mo - 5.5Cb(Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable

AMS5441B

View Details

STANDARD

Steel, Corrosion-Resistant, Bars and Forgings 13.0Cr - 2.5Ni - 5.5Co - 2.0Mo - 0.60V (0.05 - 0.09C) Vacuum Induction Plus Vacuum Consumable Electrode Melted

AMS5930B

View Details

Get Involved

Want to participate in updating this standard?

X