Browse Standards AMS5712K
Historical REVISED 2016-08-15

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution Heat Treated Precipitation Hardenable AMS5712K

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars 3.00 inches (76.2 mm) and under in nominal diameter or least distance between parallel sides, forgings, flash welded rings 3.00 inches (76.2 mm) and under in nominal radial thickness, and stock of any size for forging, flash welded rings, or heading (see 8.5).
AMS5712L
2022-08-17
Latest
Revised
AMS5712K
2016-08-15
Historical
Revised
AMS5712J
2012-01-26
Historical
Reaffirmed
AMS5712F
2011-08-15
Historical
Reaffirmed
AMS5712H
2000-07-01
Historical
Revised
AMS5712G
1995-02-01
Historical
Revised
AMS5712E
1985-10-01
Historical
Revised
AMS5712D
1983-07-01
Historical
Revised
AMS5712C
1977-01-01
Historical
Revised
AMS5712B
1966-09-01
Historical
Revised
AMS5712A
1966-03-01
Historical
Revised
AMS5712
1960-06-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings Ni - 18Cr - 2.8Mo - 5.5Cb(Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable

AMS5441B

View Details

STANDARD

Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1775 °F (968 °C) Solution and Precipitation Heat Treated

AMS5663P

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 7.0Fe - 2.5Ti - 1.0Cb (Nb) - 0.70Al 2100 °F (1149 °C) Solution and Precipitation Heat Treated

AMS5668K

View Details

Get Involved

Want to participate in updating this standard?

X