Browse Standards AMS5713K
Historical REVISED 2016-08-17

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution and Precipitation Heat Treated AMS5713K

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars 3.00 inches (76.2 mm) and under in nominal diameter or least distance between parallel sides, forgings, flash welded rings 3.00 inches (76.2 mm) and under in nominal radial thickness, and stock of any size for forging, flash welded rings, or heading (see 8.5).
AMS5713L
2022-08-17
Latest
Revised
AMS5713K
2016-08-17
Historical
Revised
AMS5713J
2012-10-11
Historical
Reaffirmed
AMS5713H
2000-08-01
Historical
Revised
AMS5713G
1994-07-01
Historical
Revised
AMS5713F
1989-07-01
Historical
Revised
AMS5713E
1985-10-01
Historical
Revised
AMS5713D
1983-07-01
Historical
Revised
AMS5713C
1977-01-01
Historical
Revised
AMS5713B
1966-09-01
Historical
Revised
AMS5713A
1966-03-01
Historical
Revised
AMS5713
1960-06-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Nickel-Iron Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 42.5Ni - 12.5Cr - 5.8Mo - 2.9Ti - 0.015B - 35Fe Consumable Electrode or Vacuum Induction Melted Solution, Stabilization, and Precipitation Heat Treated

AMS5661G

View Details

STANDARD

Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution Heat Treated Precipitation Hardenable

AMS5712L

View Details

STANDARD

Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1775 °F (968 °C) Solution and Precipitation Heat Treated

AMS5663P

View Details

Get Involved

Want to participate in updating this standard?

X