Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 °F (954 °C) Solution, Stabilization, and Precipitation Heat Treated
AMS5703E
Cobalt Alloy, Corrosion and Heat-Resistant, Bars, Forging Stock, Forgings, and Rings 52Co – 20Cr – 10Ni – 15W
AMS5759M
Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings, 21Cr - 20Ni - 20Co - 3.0Mo - 2.5W - 1.0(Cb+Ta) - 0.15N - 32Fe Solution Heat Treated