Browse Standards AMS5726B
Historical REAFFIRMED 2000-08-01

Steel, Corrosion and Heat Resistant, Bars and Wire 15Cr 25.5Ni 1.2Mo 2.1Ti 0.006B 0.30V 1800°F (982°C) Solution Heat Treated and Work-Strengthened Consumable Electrode Melted 200 ksi (1379 MPa) Tensile Strength AMS5726B

This specification covers a corrosion and heat resistant steel in the form of work-strengthened bars and wire 1-1/4 inch (31.8 mm) and under in nominal diameter of least distance between parallel sides.

These products have been used typically for parts, such as fasteners, requiring room-temperature minimum tensile strength of 200 ksi (1379 MPa) after precipitation heat treatment for use up to 1000 degrees F (538 °C) and having oxidation resistance up to 1200 °F (649 °C), but usage is not limited to such applications.

AMS5726E
2015-12-02
Latest
Reaffirmed
AMS5726D
2006-08-14
Historical
Revised
AMS5726C
2001-04-01
Historical
Revised
AMS5726B
2000-08-01
Historical
Reaffirmed
AMS5726A
1984-07-01
Historical
Revised
AMS5726
1977-01-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.

Get Involved

Want to participate in updating this standard?

X