Browse Standards AMS5726E
Historical REVISED 2015-12-02

Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V 1800 °F (982 °C) Solution Heat Treated and Work-Strengthened Consumable Electrode Remelted 200 ksi (1379 MPa) Tensile Strength Capability AMS5726E

This specification covers a corrosion and heat-resistant steel in the form of work-strengthened bars and wire 1-1/4 inches (31.8 mm) and under in nominal diameter or least distance between parallel sides.
AMS5726F
2023-03-20
Latest
Revised
AMS5726E
2015-12-02
Historical
Reaffirmed
AMS5726D
2006-08-14
Historical
Revised
AMS5726C
2001-04-01
Historical
Revised
AMS5726B
2000-08-01
Historical
Reaffirmed
AMS5726A
1984-07-01
Historical
Revised
AMS5726
1977-01-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 °F (982 °C) Solution Treated and Work-Strengthened Capable of 160 ksi (1103 MPa) Tensile Strength

AMS5853D

View Details

STANDARD

Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 °F (982 °C) Solution Treated and Work-Strengthened Capable of 160 ksi (1103 MPa) Tensile Strength

AMS5853D

View Details

STANDARD

Steel, Corrosion Resistant, Bars, Wire, and Forgings 13Cr (0.30–0.40C) (51420) Annealed

AMS5621G

View Details

Get Involved

Want to participate in updating this standard?

X