Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening AMS5841G

This specification covers a high strength, corrosion and heat-resistant cobalt-nickel-chromium alloy in the form of bars (see 8.4).
AMS5841G
2022-02-03
Latest
Reaffirmed
AMS5841F
2011-09-13
Historical
Revised
AMS5841E
2006-08-03
Historical
Revised
AMS5841D
2000-10-01
Historical
Revised
AMS5841C
1994-07-01
Historical
Revised
AMS5841B
1989-07-01
Historical
Revised
AMS5841A
1983-07-01
Historical
Revised
AMS5841
1977-03-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Exposure Levels of UV Radiation in Nondestructive Inspection Processes

AIR4964

View Details

STANDARD

Copper-Nickel Alloy Wire and Ribbon, 77.5Cu - 22.5Ni

AMS4732D

View Details

STANDARD

Alloy Sheet and Strip, Corrosion and Heat Resistant Cobalt Base 20Cr 20Ni 4Mo 4W 4Cb

AMS5534B

View Details

Get Involved

Want to participate in updating this standard?

X