Browse Standards AMS5853
Historical REAFFIRMED 2011-08-15

Steel, Corrosion and Heat Resistant, Bars and Wire 15Cr 25.5Ni 1.2Mo 2.1Ti 0.006B 0.30V, Consumable Electrode Melted 1800°F (982°C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength AMS5853

This specification covers a corrosion and heat resistant steel in the form of work-strengthened bars and wire 1-1/4 inches (31.8 mm) and under in nominal diameter or least distance between parallel sides.

These bars and wire have been used typically for parts, such as fasteners, requiring room- temperature minimum tensile strength of 160 ksi (1103 MPa) after precipitation heat treatment for use up to 1000 °F (538 °C) and having oxidation resistance up to 1200 °F (649 °C), but usage is not limited to such applications.

AMS5853D
2019-02-04
Latest
Revised
AMS5853C
2012-04-13
Historical
Reaffirmed
AMS5853
2011-08-15
Historical
Reaffirmed
AMS5853B
2000-10-01
Historical
Revised
AMS5853A
2000-08-01
Historical
Reaffirmed

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 17Cr (430) Annealed

AMS5627H

View Details

STANDARD

Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings, 12Cr Ferrite Controlled, Annealed

AMS5612K

View Details

STANDARD

Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings 13Cr - 2.0Ni - 3.0W Annealed

AMS5616M

View Details

Get Involved

Want to participate in updating this standard?

X