Browse Standards AMS5853C
Historical REAFFIRMED 2012-04-13

Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 °F (982 °C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength AMS5853C

This specification covers a corrosion and heat-resistant steel in the form of work-strengthened bars and wire, 1-1/4 inches (31.8 mm) and under in nominal diameter or least distance between parallel sides.
AMS5853D
2019-02-04
Latest
Revised
AMS5853C
2012-04-13
Historical
Reaffirmed
AMS5853
2011-08-15
Historical
Reaffirmed
AMS5853B
2000-10-01
Historical
Revised
AMS5853A
2000-08-01
Historical
Reaffirmed

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion Resistant, Bars and Wire 18Cr - 9.0Ni (302) Solution Heat Treated, Cold Drawn and Stress Relieved 125 ksi (862 MPa) Tensile Strength

AMS5637J

View Details

STANDARD

Steel, Corrosion and Heat Resistant, Wire 18Cr - 11.5Ni - 0.70Cb (Nb) (347) Solution Heat Treated

AMS5674F

View Details

STANDARD

Steel, Corrosion-Resistant, Sheet, Strip, and Plate 18Cr - 9.0Ni (302) Cold Rolled, 1/4 Hard, 125 ksi (862 MPa) Tensile Strength

AMS5903C

View Details

Get Involved

Want to participate in updating this standard?

X