Browse Standards AMS5854C
Current REVISED 2015-12-02

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Rings 61Ni - 20.5Cr - 8.5Mo - 3.4Cb(Nb) - 1.3Ti - 5.0Fe Consumable Electrode or Vacuum Induction Melted Solution Heat Treated AMS5854C

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, wire, forgings, flash welded rings, and extrusions 4 inches (102 mm) and under in nominal diameter or least distance between parallel sides, and stock for forging or flash welded rings.
AMS5854C
2015-12-02
Latest
Revised
AMS5854B
2010-05-17
Historical
Revised
AMS5854A
2006-04-20
Historical
Reaffirmed
AMS5854
1995-05-01
Historical
Reaffirmed

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings Ni - 18Cr - 2.8Mo - 5.5Cb(Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable

AMS5441B

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings Ni - 18Cr - 2.8Mo - 5.5Cb(Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated

AMS5442B

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 °F (954 °C) Solution, Stabilization, and Precipitation Heat Treated

AMS5703E

View Details

Get Involved

Want to participate in updating this standard?

X