Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable
AMS5747E
Iron-Nickel Alloy, Bars, Forgings, and Rings 42Fe - 37.5Ni - 14Co - 4.8Cb (Nb) - 1.6Ti Solution Heat Treated, Precipitation Hardenable Multiple Melted, High Temperature, Low Expansion
AMS5884E
Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip, and Plate 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated
AMS5597H