Browse Standards AMS5907A
Historical Revised 2000-11-01

Steel, Corrosion and Heat Resistant, Sheet, Strip, and Plate 17cr 12ni 2.5mo (SAE 30316) Cold Rolled, 1/4 Hard, 125 Ksi (862 Mpa) Tensile Strength AMS5907A

This specification covers a corrosion and heat resistant steel in the form of sheet, strip, and plate.

These products have been used typically in aircraft structural components requiring moderate forming and bending during fabrication and where corrosion and heat resistance up to 1600 degrees F (871 degrees C) is required, but usage is not limited to such applications. At elevated temperatures, strength of this steel is slightly higher than, and oxidation resistance is similar to, that of the 18-8 type steels.

Mechanical properties specified herein are obtained by cold working (strain hardening) and not by heat treatment. Therefore, the cold-worked product should not be heated to a temperature which adversely affects the mechanical properties of corrosion resistance before, during, or after fabrication.

AMS5907B
2012-04-16
Latest
Reaffirmed
AMS5907A
2000-11-01
Historical
Revised
AMS5907
2000-08-01
Historical
Reaffirmed

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 18% off list price.
Login to see discount.
Special Offer: Purchase more aerospace standards and aerospace material specifications and save! AeroPaks off a customized subscription plan that lets you pay for just the documents that you neeed, when you need them.

Get Involved

Want to participate in updating this standard?

X