Browse Standards AMS6317G
Historical Revised 2003-01-22

Steel Bars and Forgings 1.8ni 0.25mo (0.38-0.43c) (4640) Heat Treated, 125 Ksi (862 Mpa) Tensile Strength AMS6317G

This specification covers an aircraft-quality, low-alloy steel in the form of heat treated bars and forgings.

These products have been used typically for parts with sections 1.0 inch (25 mm) and under in nominal thickness requiring a minimum tensile strength of 125 ksi (862 MPa), but usage is not limited to such applications.

AMS6317K
2017-08-24
Latest
Revised
AMS6317J
2012-11-05
Historical
Revised
AMS6317H
2007-10-16
Historical
Revised
AMS6317G
2003-01-22
Historical
Revised
AMS6317F
1995-05-01
Historical
Reaffirmed
AMS6317E
1986-01-01
Historical
Revised
AMS6317D
1978-10-16
Historical
Revised
AMS6317C
1971-11-15
Historical
Revised
AMS6317B
1945-07-01
Historical
Revised
AMS6317A
1942-03-01
Historical
Revised
AMS6317
1939-12-04
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 18% off list price.
Login to see discount.
Special Offer: Purchase more aerospace standards and aerospace material specifications and save! AeroPaks off a customized subscription plan that lets you pay for just the documents that you neeed, when you need them.

Get Involved

Want to participate in updating this standard?

X