Browse Standards AMS6317L
Current REVISED 2022-08-09

Steel Bars and Forgings 1.8Ni - 0.25Mo (0.38 - 0.43C) (4640) Heat Treated, 125 ksi (862 MPa) Tensile Strength AMS6317L

This specification covers an aircraft-quality, low-alloy steel in the form of heat treated bars and forgings 1.00 inches (25.4 mm) and under in nominal cross section or diameter and for hexagonal shapes, least distance between parallel sides.
AMS6317L
2022-08-09
Latest
Revised
AMS6317K
2017-08-24
Historical
Revised
AMS6317J
2012-11-05
Historical
Revised
AMS6317H
2007-10-16
Historical
Revised
AMS6317G
2003-01-22
Historical
Revised
AMS6317F
1995-05-01
Historical
Reaffirmed
AMS6317E
1986-01-01
Historical
Revised
AMS6317D
1978-10-16
Historical
Revised
AMS6317C
1971-11-15
Historical
Revised
AMS6317B
1945-07-01
Historical
Revised
AMS6317A
1942-03-01
Historical
Revised
AMS6317
1939-12-04
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Aluminum Alloy, Castings 4.5Cu - 0.70Ag - 0.30Mn - 0.25Mg - 0.25Ti (A201.0-T4) Solution Heat Treated and Naturally Aged

AMS4223E

View Details

STANDARD

COUPLING, SHEET METAL, 40° V-BAND, STANDARD LATCH

AS1960/1A

View Details

STANDARD

Anodic Treatment of Magnesium Alloys Acid Type, Full Coat

AMS2478E

View Details

Get Involved

Want to participate in updating this standard?

X