Steel, Bars, and Forgings 0.50Cr - 0.55Ni - 0.25Mo (0.38 - 0.43C) (SAE 8740) Heat Treated, 105 ksi (724 MPa) Tensile Strength AMS6325L

This specification covers an aircraft-quality, low-alloy steel in the form of heat treated bars and forgings.
AMS6325L
2020-04-10
Latest
Revised
AMS6325K
2015-12-20
Historical
Revised
AMS6325J
2010-04-19
Historical
Revised
AMS6325H
2004-10-18
Historical
Revised
AMS6325G
2000-09-01
Historical
Reaffirmed
AMS6325F
1988-07-01
Historical
Revised
AMS6325E
1972-11-15
Historical
Revised
AMS6325D
1966-09-30
Historical
Revised
AMS6325C
1951-06-01
Historical
Revised
AMS6325B
1945-07-01
Historical
Revised
AMS6325A
1943-04-01
Historical
Revised
AMS6325
1942-09-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.

Get Involved

Want to participate in updating this standard?

X