Browse Standards AMS6327L
Current REVISED 2017-09-22

Steel Bars and Forgings 0.50Cr - 0.55Ni - 0.25Mo (0.38 - 0.43C) (SAE 8740) Heat Treated, 125 ksi (862 MPa) Tensile Strength AMS6327L

This specification covers an aircraft-quality, low-alloy steel in the form of bars and forgings.
AMS6327L
2017-09-22
Latest
Revised
AMS6327K
2012-10-03
Historical
Revised
AMS6327J
2007-10-16
Historical
Revised
AMS6327H
2003-01-22
Historical
Revised
AMS6327G
2000-10-01
Historical
Reaffirmed
AMS6327F
1981-01-15
Historical
Revised
AMS6327E
1972-11-15
Historical
Revised
AMS6327D
1966-09-30
Historical
Revised
AMS6327C
1951-06-01
Historical
Revised
AMS6327B
1945-07-01
Historical
Revised
AMS6327A
1943-04-01
Historical
Revised
AMS6327
1942-09-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Bars, and Forgings 0.50Cr - 0.55Ni - 0.25Mo (0.38 - 0.43C) (SAE 8740) Heat Treated, 105 ksi (724 MPa) Tensile Strength

AMS6325K

View Details

STANDARD

Steel, Bars, and Forgings 0.50Cr - 0.55Ni - 0.25Mo (0.38 - 0.43C) (SAE 8740) Heat Treated, 105 ksi (724 MPa) Tensile Strength

AMS6325K

View Details

STANDARD

Steel, Heat-Resistant, Bars, Forgings, and Tubing 0.95Cr - 0.55Mo - 0.30V (0.40 - 0.50C) Vacuum Arc Remelted

AMS6305G

View Details

Get Involved

Want to participate in updating this standard?

X