Browse Standards AMS6346C
Current REVISED 2018-06-11

Steel Bars 0.95Cr - 0.20Mo (0.28 to 0.33C) (SAE 4130) Hardened and Tempered, 125 Ksi (862 MPa) Tensile Strength AMS6346C

This specification covers an aircraft-quality, low-alloy steel in the form of heat treated bars 1.50 inches (38.1 mm) and less in diameter or least distance between parallel sides.
AMS6346C
2018-06-11
Latest
Revised
AMS6346B
2013-10-04
Historical
Revised
AMS6346A
2009-06-11
Historical
Reaffirmed
AMS6346
1998-10-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Titanium Alloy, Forgings 10V - 2Fe - 3Al Consumable Electrode Melted, Single-Step Solution Heat Treated and Aged 180 ksi (1241 MPa) Tensile Strength

AMS4983G

View Details

STANDARD

Titanium Alloy, Forgings 10V - 2Fe - 3Al Consumable Electrode Melted, Single-Step Solution Heat Treated and Aged 180 ksi (1241 MPa) Tensile Strength

AMS4983G

View Details

STANDARD

Steel Tubing, Seamless 0.95Cr - 0.20Mo (0.28 - 0.33C) (SAE 4130) 125 ksi (862 MPa) Tensile Strength

AMS6361G

View Details

Get Involved

Want to participate in updating this standard?

X