Browse Standards AMS7727F
Current STABILIZED 2017-04-06

Iron-Nickel-Cobalt Alloy, Bars and Forgings 53Fe - 29Ni - 17Co Low Expansion, Glass Sealing(STABILIZED Apr 2017) AMS7727F

This specification covers an iron-nickel-cobalt alloy in the form of bars and forgings.
AMS7727F
2017-04-06
Latest
Stabilized
AMS7727E
2012-04-16
Historical
Reaffirmed
AMS7727D
2000-06-28
Historical
Revised
AMS7727C
1995-02-01
Historical
Revised
AMS7727B
1988-07-01
Historical
Revised
AMS7727A
1981-01-01
Historical
Revised
AMS7727
1964-01-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1750 °F (954 °C) Solution Heat Treated

AMS5702E

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1750 °F (954 °C) Solution Heat Treated

AMS5702E

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution and Precipitation Heat Treated

AMS5713K

View Details

Get Involved

Want to participate in updating this standard?

X