Browse Standards AMSC26074A
Historical CANCELLED 2005-02-16

Coatings, Electroless Nickel Requirements for AMSC26074A

This specification covers the requirements for electroless (autocatalytic chemical reduction) deposition of nickel-phosphorous alloy coatings on metal and composite surfaces.
AMSC26074D
2013-06-01
Latest
Stabilized
AMSC26074C
2011-07-08
Historical
Canceled
AMSC26074B
2005-10-27
Historical
Noncurrent
AMSC26074A
2005-02-16
Historical
Revised
AMSC26074
1998-08-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Electroless Nickel Coatings

AMSC26074D

View Details

STANDARD

Steel, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 17Cr - 13Ni - 2.5Mo (316L) Solution Heat Treated

AMS5507H

View Details

STANDARD

Steel, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 18Cr - 10.5Ni - 0.80Cb (347) Solution Heat Treated

AMS5512M

View Details

Get Involved

Want to participate in updating this standard?

X