Browse Standards ARP982
Historical ISSUED 1967-11-01

Minimizing Stress-Corrosion Cracking in Wrought Titanium Alloy Products ARP982

Primarily to provide recommendations concerning minimizing stress corrosion cracking in wrought titanium alloy products.
ARP982D
2020-09-21
Latest
Reaffirmed
ARP982C
2002-12-19
Historical
Reaffirmed
ARP982B
1984-04-01
Historical
Revised
ARP982A
1971-11-01
Historical
Revised
ARP982
1967-11-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Wire 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Spring Temper, Precipitation Hardenable

AMS5699G

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Wire 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe No. 1 Temper, Precipitation Hardenable

AMS5698G

View Details

STANDARD

TUBE END, WELD DESIGN STANDARD

AS1577B

View Details

Get Involved

Want to participate in updating this standard?

X