Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 57Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.006B 0.05Zr, Consumable Electrode or Vacuum Induction Melted, 995 to 1040°C Solution Heat Treated(Cancelled Mar 2003) MAM5706C

This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging, flash welded rings, or heading procured in SI (metric) units.

AMS 5706 is the inch/pound version of this MAM.

These products have been used typically for parts, such as fasteners, flanges, and rings, requiring high strength up to 815 degrees C and oxidation resistance up to 955 degrees C, particularly those parts which are formed or welded and then heat treated to develop required properties, but usage is not limited to such applications.

MAM5706C
2003-03-12
Latest
Canceled
MAM5706B
1998-07-01
Historical
Reaffirmed
MAM5706A
1989-07-01
Historical
Revised
MAM5706
1987-10-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 18% off list price.
Login to see discount.
Special Offer: Purchase more aerospace standards and aerospace material specifications and save! AeroPaks off a customized subscription plan that lets you pay for just the documents that you neeed, when you need them.

Get Involved

Want to participate in updating this standard?

X