Browse Standards AMS5737P
Current REAFFIRMED 2018-10-10

Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Tubing 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1650 °F (899 °C) Solution and Precipitation Heat Treated AMS5737P

This specification covers a corrosion and heat-resistant steel in the form of bars, wire, forgings, mechanical tubing, and stock for forging or heading.
AMS5737P
2018-10-10
Latest
Reaffirmed
AMS5737N
2000-11-20
Historical
Revised
AMS5737M
1995-05-01
Historical
Revised
AMS5737L
1989-07-01
Historical
Revised
AMS5737K
1985-04-01
Historical
Revised
AMS5737J
1983-04-01
Historical
Revised
AMS5737H
1977-01-01
Historical
Revised
AMS5737G
1976-07-01
Historical
Revised
AMS5737F
1976-01-01
Historical
Revised
AMS5737E
1971-05-01
Historical
Revised
AMS5737D
1968-11-01
Historical
Revised
AMS5737C
1966-03-01
Historical
Revised
AMS5737B
1959-11-01
Historical
Revised
AMS5737A
1959-01-01
Historical
Issued
AMS5737
1959-01-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion-Resistant, Bars, Wire, and Forgings 18Cr - 9.0Ni Free Machining

AMS5640V

View Details

STANDARD

Steel, Corrosion-Resistant, Bars, Wire, and Forgings 17Cr - 0.52Mo (0.95 - 1.20C) (440C)

AMS5630L

View Details

STANDARD

Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Tubing 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted, 1650 °F (899 °C) Solution Heat Treated

AMS5734K

View Details

Get Involved

Want to participate in updating this standard?

X