Standard STEEL SHEET AND STRIP, CORROSION RESISTANT Cold Rolled High Ductility Type 18 Chromium - 8 Nickel (185,000 T.S.) 1942-06-01 HISTORICAL AMS5519B
Standard STEEL SHEET AND STRIP, CORROSION RESISTANT 18Cr - 8Ni (Cold Rolled - 185,000 psi) 1947-09-01 HISTORICAL AMS5519C
Standard STEEL SHEET AND STRIP, CORROSION RESISTANT Cold Rolled High Ductility Type 18 Chromium - 8 Nickel (185,000 T.S.) 1941-11-01 HISTORICAL AMS5519A
Standard STEEL SHEET AND STRIP, CORROSION RESISTANT 18Cr - 8Ni (SAE 30301) Cold Rolled, 185,000 psi (1276 MPa) Tensile Strength 1979-01-01 HISTORICAL AMS5519G This specification covers a corrosion-resistant steel in the form of sheet and strip.
Standard STEEL SHEET AND STRIP, CORROSION RESISTANT 18 Chromium - 8 Nickel (Spring) 1940-01-01 HISTORICAL AMS5519
Standard STEEL SHEET AND STRIP, CORROSION RESISTANT 18Cr - 8Ni (SAE 30301) Cold Rolled, 185,000 psi (1276 MN/m2) 1971-05-01 HISTORICAL AMS5519F This specification covers a corrosion resistant steel in the form of sheet and strip.
Standard STEEL SHEET AND STRIP, CORROSION RESISTANT 18Cr - 8Ni Cold Rolled - 185,000 psi 1952-02-01 HISTORICAL AMS5519E
Standard STEEL SHEET AND STRIP, CORROSION RESISTANT 18Cr-8Ni (SAE 30302) Cold Rolled - 185,000 psi 1949-08-01 HISTORICAL AMS5519D
Standard Steel, Corrosion Resistant, Sheet and Strip 18Cr - 8Ni (SAE 30301) Cold Rolled, 185 ksi (1276 MPa) Tensile Strength 1999-01-01 HISTORICAL AMS5519L This specification covers a corrosion-resistant steel in the form of sheet and strip.
Standard STEEL, CORROSION RESISTANT, SHEET AND STRIP 18Cr - 8Ni (SAE 30301) Cold Rolled, 185 ksi (1276 MPa) Tensile Strength 1992-07-01 HISTORICAL AMS5519K This specification covers a corrosion-resistant steel in the form of sheet and strip.
Standard STEEL SHEET AND STRIP, CORROSION RESISTANT 18Cr - 8Ni (SAE 30301) Cold Rolled, 185,000 psi (1276 MPa) Tensile Strength 1990-01-01 HISTORICAL AMS5519J This specification covers a corrosion-resistant steel in the form of sheet and strip.
Standard STEEL SHEET AND STRIP, CORROSION RESISTANT 18Cr - 8Ni (SAE 30301) Cold Rolled, 185,000 psi (1275 MPa) Tensile Strength 1984-10-01 HISTORICAL AMS5519H This specification covers a corrosion-resistant steel in the form of sheet and strip.
Standard Steel, Corrosion Resistant, Sheet and Strip 18Cr – 8Ni (SAE 30301) Cold Rolled, 185 ksi (1276 MPa) Tensile Strength 2014-06-10 HISTORICAL AMS5519N This specification covers a corrosion-resistant steel in the form of sheet and strip.
Standard Steel, Corrosion Resistant, Sheet and Strip 18Cr - 8Ni (SAE 30301) Cold Rolled, 185 ksi (1276 MPa) Tensile Strength 2003-06-03 HISTORICAL AMS5519M This specification covers a corrosion-resistant steel in the form of sheet and strip.
Standard Steel, Corrosion Resistant, Sheet and Strip 18Cr - 8Ni (SAE 30301) Cold Rolled, 185 ksi (1276 MPa) Tensile Strength 2020-02-14 CURRENT AMS5519P This specification covers a corrosion-resistant steel in the form of sheet and strip 0.005 inch (0.13 mm) and over in nominal thickness (see 8.7).