Monitoring of Ring Face, Ring Side and Liner Wear in a Mack T-10 Test, using Surface Layer Activation

2007-10-29
2007-01-4002
The API has established lubricant specifications, which include standard tests for ring and liner wear. The Mack T-10 is one such test, performed on a prototype engine with Exhaust Gas Recirculation (EGR). At EOT, the liner wear is measured by profilometry, while the ring wear is measured by weight loss. It was decided to monitor the wear of the rings and liners during a full-length T10 test in order to observe the evolution of the wears and wear rates over the course of the test, by using the Surface Layer Activation (SLA) and Bulk Activation (BA) techniques. Three different radioisotopes were created, one in the liners at the turnaround zone, one in the chromium-containing coating on the ring faces, and one in the iron bulk of the rings. This enabled us to observe the wear characteristics of these three components separately. In particular, we were able to separate the face and side ring wears, which cannot be done with simple weight-loss measurements.
X