Technical Paper

Material Compatibilities of Biodiesels with Elastomers, Metals and Plastics in a Diesel Engine

2009-11-02
2009-01-2799
The effects of biodiesel on the swelling of the elastomers and plastics and the corrosion of metals are studied by the immersion tests. The results indicate that biodiesels make little corrosion effect on aluminum, steel and little swelling impact on plastics, but a significant corrosion may be taken place on cooper and brass for some sourced biodiesels. For nitrile-butadiene rubber, the variation of swelling properties in biodiesels is slightly higher than that in diesel. For the non-diesel-resistant elatomers, the variation of swelling properties is lower than those in diesel. The production process and biodiesel source have an influence on the result of elastomer swelling and corrosion. The relationship between the impact of biodiesel on materials and biodiesels properties are also discussed.
Technical Paper

Compatibility of Biodiesels and Their Blends with Typical Rubbers and Copperish Metals

2010-04-12
2010-01-0476
The swelling of ‘O’ rings of 3 typical rubbers (NBR, FKM, EPDM) and the corrosion of 2 typical copperish metal pieces (Copper, Brass) were investigated. The fuel samples included 14 kinds of biodiesels, 1 kind of diesel, and 4 kinds of blends respectively for 2 kinds of biodiesels. The changes in mass and size of ‘O’ rings were measured with an electronic balance and a vernier caliper. The surface corrosion of copperish metals was recorded with photos. It was found that the swelling of NBR in pure biodiesels were generally larger than those in diesel. The mass and size of FKM almost did not change in both pure biodiesels and diesel. The swelling of EPDM became less in pure biodiesels than that in diesel. When the blend ratios of biodiesels were less than 10%, the change rates in mass, inner diameter and section diameter of NBR, FKM and EPDM were similar between blended fuels and diesel.
Technical Paper

Effect of Nozzle Geometry on Macroscopic Behavior of Diesel Spray in the Near-Nozzle Field

2013-04-08
2013-01-1587
In this study, the orifice inlet rounding radii of four diesel nozzles with different hydro erosive grinding time were measured based on the x-ray CT scan technology provided by Shanghai Synchrotron Radiation Facility (SSRF), and a wide parametrical study of the spray macroscopic behavior in the first 18 mm from the nozzle tip have been carried out with high speed camera. And then the influence of orifice inlet rounding radius on the spray behavior in the near-nozzle field was thoroughly investigated. The investigation results show that: the mean values of orifice inlet rounding radii of different nozzles are measured to be on the order of 21.5-56.8 μm. Although the spray tip penetrations of different nozzles tend to increase with the hydro erosive grinding time through statistical analyzing method, the variations of penetration from nozzles are less than 15% according to different hydro erosive grinding timing.
Technical Paper

Fatigue Endurance Limit of Fasteners in Automotive Application

2022-03-29
2022-01-0260
Fasteners, commonly used in automotive industry, play an important role in the safety and reliability of the vehicle structural system. In practical application, bolted joints would never undergo fully reversed loading; there always will be positive mean stress on bolt. The mean stress has little influence on the fatigue life if the maximum stress is lower than a threshold which is near the yield stress of the bolt. However, when the sum of the mean stress and the stress amplitude exceeds the threshold, the endurance limit stress amplitude decreases fast as the mean stress increases. The purpose of this paper is to research the fatigue endurance limit of a fastener and establish the threshold for safe design in automotive application. In order to obtain the fatigue endurance limit at different mean stress levels, various mechanical tests were performed on M12x1.75 and M16x1.5 Class 10.9 fasteners using MTS test systems.
Technical Paper

Numerical Simulation of Surface Temperature Fluctuation and Thermal Barrier Coating at the Piston Top for a Diesel Engine Performance Improvement

2021-04-06
2021-01-0229
Low heat rejection (LHR) combustion has been recognized as a potential technology for further fuel economy improvement. This paper aims to simulate how the piston top’s thermal barrier coating affects the engine’s thermal efficiency and emissions. Accordingly, a Thin-wall heat transfer model in AVL Fire software was employed. The effects of increasing the piston top surface temperature, comparing different thermal barrier coating material, were simulated at the engine’s rated power operating point, so as the piston top’s surface roughness. In comparison to a standard diesel engine, the indicated thermal efficiency (ITE) could increase by 0.4% when the surface temperature of the piston top changed from 575K to 775K.