Technical Paper

Next Generations of Gasoline Particulate Filters for Catalyzed Applications

2024-04-09
2024-01-2384
Gasoline particulate filters (GPF) have become a standard aftertreatment component in Europe, China, and since recently, India, where particulate emissions are based on a particle number (PN) standard. The anticipated evolution of regulations in these regions towards future EU7, CN7, and BS7 standards further enhances the needs with respect to the filtration capabilities of the GPFs used. Emission performance has to be met over a broader range in particle size, counting particles down to 10nm, and over a broader range of boundary conditions. The requirements with respect to pressure drop, aiming for as low as possible, and durability remain similar or are also enhanced further. To address these future needs new filter technologies have been developed. New technologies for uncatalyzed GPF applications have been introduced in our previous publications.
Technical Paper

Evaluation of Uncoated Gasoline Particulate Filter Performance for US EPA MY27+ Particulate Mass Emissions Regulation

2024-04-09
2024-01-2383
The gasoline particulate filter (GPF) represents a practical solution for particulate emissions control in light-duty gasoline-fueled vehicles. It is also seen as an essential technology in North America to meet the upcoming US EPA tailpipe emission regulation, as proposed in the “Multi-pollutant Rule for Model Year 2027”. The goal of this study was to introduce advanced, uncoated GPF products and measure their particulate mass (PM) reduction performance within the existing US EPA FTP vehicle testing procedures, as detailed in Code of Federal Regulations (CFR) part 1066. Various state-of-the-art GPF products were characterized for their microstructure properties with lab-bench checks for pressure drop and filtration efficiency, then pre-conditioned with an EPA-recommended 1500 mile on-road break-in, and finally were tested on an AWD vehicle chassis-dyno emissions test cell at both 25°C and -7°C ambient conditions.
Technical Paper

Challenges of Particulate Number above 10nm Emissions for a China 6 Compliant Vehicle to Meet Future Regulation

2023-04-11
2023-01-0377
As the official proposal for emission regulation Euro 7 has been released by European Commission, PN above 10nm is taken into consideration for the ultrafine particulate emissions control. The challenges of GPF filtration efficiency emerge for the light-duty manufactures to meet the future emission standards. In the present study, a China 6 compliant vehicle was tested to reveal its performance over the China 6 standards and potential to meet the upcoming Euro 7. Three GPF product types (Gen 1, Gen 2, and concept Gen 3) were mounted to the tested vehicle. WLTC tests were conducted on chassis dynamometer in laboratory as well as a self-designed aggressive cycle (“Base Cycle”) tests. To explore the GPFs performance for PN emissions above 10nm against the proposed limit 6.0E11 #/km, PN emission above 10nm were measured in our laboratory tests for both engine out and tailpipe as well as the PN emission above 23nm.
Technical Paper

Calculation Methods Impact on Real-Driving-Emissions Particulate Number Evaluation: Moving Averaging Window in China 6 vs. Raw Mileage Averaging in Euro 6d

2022-03-29
2022-01-0567
RDE test has been introduced to the light-duty vehicle certification process in both China 6 and Euro 6d standards. The RDE test shall be performed on-road with PEMS, which is developed to complement the current laboratory certification of vehicles and ensure cars to deliver low emissions under more realistic on-road driving conditions. Particulate matter has been highly perceived as a significant contributor to human health risks and thus strictly regulated globally. For the RDE evaluation, the MAW method used by the China 6 standard is usually found less stringent than the RMA method used by the Euro 6d standard. In the present study, both of the MAW and RMA methods were applied to different driving cycles and operating conditions, which met the general RDE test requirements, yet resulted in different evaluated PN results.
Journal Article

Effect of Decoration on Windshield Impact Resistance and Novel Decoration Solution Compatible with Chemical Strengthening

2022-03-29
2022-01-0263
Vehicle windshields typically include a black decorative pattern around their periphery and other regions. Examination of field failed parts has shown that windshields often break from impacts in these decoration zones; often with the fracture initiating from the decoration material itself. In this work, the effect of different glazing decoration materials on glass strength and laminate impact resistance was evaluated. The decoration materials investigated included traditional inorganic enamel frit, an organic ink, and a new enamel frit that is compatible with glass chemical strengthening. Ring-on-Ring strength tests were conducted and showed that inorganic enamel frit reduces strength of glass by over 50% compared to undecorated glass, while organic inks do not adversely affect strength. Tests of a newly developed decoration frit material, compatible for chemical strengthening processes, showed strength levels that were on par with undecorated, unstrengthened glass.
Technical Paper

Characterization and Quantification of In-Service Windshield Fracture Mechanisms and Evaluation of Laminate Sharp Impact Resistance as a Function of Construction

2020-04-14
2020-01-0607
Examination of field-fractured windshields was conducted for purposes of determining the principle fracture mechanisms experienced in-use. Samples for the study were gathered both in the United States (New York) and in Europe (France) to explore whether the primary causes of failure were similar for the different geographic regions. In total, over two hundred individual field-fractures were obtained and examined for the study. Detailed fracture analysis of the parts was performed, and multiple fracture mechanisms were identified and quantified. It was found that the two most frequently observed failure modes were common for both regions with the most frequent cause (~70%) of fractures being due to sharp contact of the exterior ply, while Hertzian cone cracking of the outer ply was the second leading cause (~20%). Several other modes were also identified. Given that sharp impact fracture was the dominant observed failure mode, a high-speed, sharp impact test method was developed.
Technical Paper

Effect of Ash on Gasoline Particulate Filter Using an Accelerated Ash Loading Method

2018-04-03
2018-01-1258
Gasoline particulate filter (GPF) is considered a suitable solution to meet the increasingly stringent particle number (PN) regulations for both gasoline direct injection (GDI) and multi-port fuel injection (MPI) engines. Generally, GDI engines emit more particulate matter (PM) and PN. In recent years, GDI engines have gained significant market penetration in the automobile industry owing to better fuel economy and drivability. In this study, an accelerated ash loading method was tested by doping lubricating oil into the fuel for a GDI engine. Emission tests were performed at different ash loads with different driving cycles and GPF combinations. The results showed that the GPF could significantly reduce particle emissions to meet the China 6 regulation. With further ash loading, the filtration efficiency increased above 99% and the effects on fuel consumption and backpressure were found to be limited, even with an ash loading of up to 50 g/l.
Technical Paper

Optical Advantages of Thin Window Hybrid Windshields

2018-04-03
2018-01-0468
The adoption of head-up displays (HUDs) is increasing in modern automobiles. Yet integrating this technology into vehicles with standard windshield (WS) laminates can create negative effects for drivers, primarily due to the thickness of glass used. The double ghosting in HUD images is typically overcome by employing a wedged PVB between the two glass plies of the laminate. Another solution is to reduce the thickness of the glass without impacting the overall windshield toughness. Although this still requires the use of a wedged PVB to eliminate HUD ghosting, the thinner glass provides opportunity to increase the image size. However, reducing the thickness of a soda-lime glass (SLG) ply or plies in a conventional soda-lime glass (SLG) laminate can significantly impact the robustness of the laminate to external impact events.
Technical Paper

Assessment of Lightweight Automotive Glass Solutions on Interior Noise Levels & Sound Quality

2017-06-05
2017-01-1814
The automotive industry continues to develop technologies for reducing vehicle fuel consumption. Specifically, vehicle lightweighting is expected to be a key enabler for achieving fleet CO2 reduction targets for 2025 and beyond. Hybrid glass laminates that incorporate fusion draw and ion exchange innovations are thinner and thereby, offer more than 30% weight reduction compared to conventional automotive laminates. These lightweight hybrid laminates provide additional benefits, including improved toughness and superior optics. However, glazing weight reduction leads to an increase in transmission of sound through the laminates for certain frequencies. This paper documents a study that uses a systematic test-based approach to understand the sensitivity of interior vehicle noise behavior to changes in acoustic attenuation driven by installation of lightweight glass.
Journal Article

Reliability Evaluation of Thin, Lightweight Laminates for Windshield Applications

2016-04-05
2016-01-1401
The use of lightweight materials to produce automotive glazing is being pursued by vehicle manufacturers in an effort to improve fuel economy. As glazing’s become thinner, reduced rigidity means that the critical flaw size needed to create fracture becomes much smaller due to increased strain under load or impact. This paper documents experiments focused on the impact performance of several alternative thin laminate constructions under consideration for windshield applications (including conventional annealed soda-lime glass as well as laminates utilizing chemically strengthened glass), for the purpose of identifying new and unique failure modes that result from thickness reduction. Regulatory impact tests and experiments that focused on functional performance of laminates were conducted. Given the increased sensitivity to flaw size for thin laminates, controlled surface damage was introduced to parts prior to conducting the functional performance tests.
Technical Paper

Ultra Thin Wall Substrates - Trends for Performance in FTP and US06 Tests

2002-03-04
2002-01-0356
This paper compares the emissions performance of four ultra thin wall ceramic substrates with standard wall thickness product on a chassis dynamometer for two different substrate volumes. This comparison helps establish performance trends and provides useful information for selection of substrates in designing catalytic converter systems. This experimental study tests and compares four ultra thin wall products (400/4, 600/3, 600/4, and 900/2) with a standard wall product (400/6.5) at two different substrate volumes. Engine bench aging is used to simulate typical aged conditions. Temperature data as well as second by second and bag emissions data for hydrocarbons, carbon monoxide and oxides of nitrogen were used to evaluate the relative performances of the substrates. The US FTP and US06 driving cycles were used as protocols for the comparison. Results suggest that lower bulk density and higher geometric surface area interact to lead to lower emissions.
Technical Paper

Performance and Durability Evaluation of Continuously Regenerating Particulate Filters on Diesel Powered Urban Buses at NY City Transit - Part II

2002-03-04
2002-01-0430
In urban areas, particulate emission from diesel engines is one of the pollutants of most concern. As a result, particulate emission control from urban bus diesel engines using particle filter technology is being evaluated at several locations in the US. A project entitled, “Clean Diesel Vehicle Air Quality Project” has been initiated by NY City Transit under the supervision of NYSDEC and with active participation from several industry partners. Under this program, 25 NY City transit buses with DDC Series 50 engines have been equipped with continuously regenerating diesel particulate filter systems and have been operating with ultra low sulfur diesel (< 30 ppm S) in transit service in Manhattan since February 2000. These buses were evaluated over a 9 month period for operations, maintainability and durability of the particulate filter.
Technical Paper

Evaluation of SoftMountSM Technology for Use in Packaging UltraThinwall Ceramic Substrates

2002-03-04
2002-01-1097
Quantitative in-use pressure measurements were taken from packaging ceramic substrates with the SoftMountSM technology and two more traditional technologies, stuffing and tourniquet. Each technology was assessed using four separate mat materials. Mat selection enhanced the application of the SoftMountSM technology through the reduced pressures applied to the substrate during packaging. High temperature and low temperature thermal cycling studies were performed on the canned converters for the three packaging technologies so that an evaluation could be made of converter durability. The SoftMountSM packaging technology yielded the lowest pressures of all the processes studied, regardless of mat type. The laminar hybrid mat evaluated yielded the best combination of pressure and durability performance. Low temperature residual shear strengths following thermal cycling of the converters showed good correlation between the SoftMountSM technology and the stuffing method.
Technical Paper

Shear Strength of Cordierite Ceramic Catalyst Supports

2001-03-05
2001-01-0935
An analytical model for estimating shear and bending stresses during canning of cordierite ceramic catalyst supports is presented. These stresses arise when the radial pressure distribution is nonuniform due, primarily, to variations in gap bulk density (GBD ) of intumescent mat around the perimeter of the substrate. Variations in GBD can occur during canning, regardless of the canning technique, due to anisotropic can stiffness or component tolerances or mat overlap. The model helps relate shear and bending stresses to substrate size and orientation, elastic modulii, cell size and wall porosity. If these stresses approach the corresponding strength of substrate, a shear crack may develop during or after the canning process depending on the magnitude of stress. A special test fixture was developed to measure the shear strength of ceramic catalyst supports, with different cell sizes, before and after the application of washcoat.
Technical Paper

Diesel Emission Control - Last 12 Months in Review

2000-10-16
2000-01-2817
The key diesel emission control papers of the last 12 months have been summarized. In addition, the emerging US and European light-duty and heavy-duty tailpipe regulations are compared. Results are reported on light-duty diesel filtration regeneration systems and experiences, including effects of ash build-up and some recent modeling work. On the heavy-duty side, optimization of SCR catalysts and systems are described, as well as experiences with the first integrated SCR/filter systems, which are already achieving “Euro V” 2008 standards. An update on NOx adsorbers is also provided. The results with new NOx formulations are described, as well as the system performance in a light-duty diesel application.
Technical Paper

Effect of Temperature on Biaxial Strength of Automotive Windshields

2000-10-03
2000-01-2722
This paper focuses on the effect of temperature on biaxial strength of curved, symmetrically laminated, automotive windshields. In view of their aspheric curvature, the measurement of biaxial strength requires a special ring-on-ring test fixture with compliant loading and support rings. The key factors that affect strength are (i) fatigue behavior of surface flaws, (ii) expansion mismatch between glass and PVB interlayer, and (iii) interfacial bond integrity. These, in turn, depend on the operating temperature which for automotive windshields can range from −40°C in winter to +50°C in summer. The data show that the biaxial strength is 21% higher at −40°C and 28% lower at +50°C than that at room temperature. An assessment of fatigue and interfacial bond integrity shows that strength changes of these magnitudes are predominantly caused by residual stresses arising from expansion mismatch between glass and PVB interlayer.
Technical Paper

Measurement of Biaxial Strength of New vs. Used Windshields

2000-10-03
2000-01-2721
This paper presents the strength data for conventional automotive windshields in both the new and used conditions. More specifically, the biaxial strength of outer surface of curved and symmetrically laminated windshield, measured in biaxial flexure, is reported. The relative contributions of inplane membrane stress, which can be significant for new windshields, and bending stress are quantified with the aid of strain gauge rosettes mounted on both the outer and inner surfaces of windshield. The strength distribution for new and used windshields, based on Weibull distribution function, is found to be multimodal indicating more than one family of surface flaws. Depending on handling damage during manufacturing, assembly and installation processes, the low strength region of new windshields can approach that of used windshields with 50,000+ road miles!
Technical Paper

A New Converter Concept Providing Improved Flow Distribution and Space Utilization

1999-03-01
1999-01-0768
A new converter concept is introduced, which utilizes the additional space in the inlet cone of the converter. An optimized design is obtained by the application of computational fluid dynamics (CFD) and flow distribution measurements, resulting in up to 20% improved flow distribution through the substrate. In addition, the volume of the converter can be increased by approximately 15% using the same space envelope. Durability tests of the converter system have been performed using a thermal cycling test on an engine test bench for 135 hours. No deterioration of the substrate or mounting system occurred. The emissions performance was evaluated on a stationary dynamometer. The impact of the flow distribution on the temperature field and the conversion behavior during light-off and steady state operation were investigated. Under the current testing conditions, no differences in light-off behavior were determined, despite significant differences in the temperature field.
Technical Paper

Fatigue and Performance Data for Advanced Thin Wall Ceramic Catalysts

1998-02-23
980670
With stricter emissions standards, low back pressure requirements, and 100,000 mile durability specifications, ceramic catalysts have undergone significant developments over the past few years. The thrust in the ceramics area has centered on thin-wall structures to minimize back pressure and on high cell density for rapid light-off in close-coupled applications. The thin-wall structures are extruded from low expansion cordierite ceramic with adequate strength and thermal shock resistance equivalent to those of standard cordierite substrate. Examples of thin-wall substrate include 350XT which is extruded from a very low expansion dense cordierite ceramic, and 400/4 and 600/4 cell structures extruded from a low expansion modified cordierite ceramic. This paper will focus on the high fatigue resistance, excellent conversion efficiency, and low back pressure of 350 XT substrates with advanced washcoat system.
Technical Paper

Advances of Durability of Ceramic Converter Systems

1996-10-01
962372
Governing bodies world-wide are setting increasingly tighter emission standards to help improve air quality. US and Californian LEV/ULEV standards are pace setting, European Stage II legislation has just become effective. In Brazil, the upcoming 1997 standards are also demanding for tighter emission control. The monolithic ceramic honeycomb catalytic converter -for more than the past 20 years- has been a reliable key element in the automotive emission control systems. In order to help meet tightened emission regulation as well to satisfy even more stringent durability requirement, an advanced thinwall ceramic Celcor XT has been developed for increased geometric surface area and reduced backpressure. The product properties as well as FTP and ECE emission and durability test results are being described in this paper. Converter system durability is also determined by robust canning and mounting systems. A durable mounting concept, especially for preconverters, is being described.