Refine Your Search

Topic

Search Results

Technical Paper

Optical Advantages of Thin Window Hybrid Windshields

2018-04-03
2018-01-0468
The adoption of head-up displays (HUDs) is increasing in modern automobiles. Yet integrating this technology into vehicles with standard windshield (WS) laminates can create negative effects for drivers, primarily due to the thickness of glass used. The double ghosting in HUD images is typically overcome by employing a wedged PVB between the two glass plies of the laminate. Another solution is to reduce the thickness of the glass without impacting the overall windshield toughness. Although this still requires the use of a wedged PVB to eliminate HUD ghosting, the thinner glass provides opportunity to increase the image size. However, reducing the thickness of a soda-lime glass (SLG) ply or plies in a conventional soda-lime glass (SLG) laminate can significantly impact the robustness of the laminate to external impact events.
Technical Paper

Effect of Cell Geometry on Emissions Performance of Ceramic Catalytic Converters

2002-03-04
2002-01-0354
More stringent emissions regulations, space limitations for catalytic converters in modern automotive applications, and new engine technologies constitute design challenges for today's engineers. In that context high cell density thinwall and ultrathinwall ceramic substrates have been designed into advanced catalytic converters. Whereas the majority of these substrates have a square cell geometry, a potential for further emissions improvement has been predicted for hexagonal cell structures. In order to verify these predictions, a ceramic substrate has been developed combining the features of high cell density, ultrathin cell walls, and hexagonal cell structure. Based on modeling data, the actual cell density and wall thickness of the hexagonal cell substrate will be defined. The performance of that substrate will be assessed by comparing experimental emissions results using two modern Volkswagen engines.
Technical Paper

Ultra Thin Wall Substrates - Trends for Performance in FTP and US06 Tests

2002-03-04
2002-01-0356
This paper compares the emissions performance of four ultra thin wall ceramic substrates with standard wall thickness product on a chassis dynamometer for two different substrate volumes. This comparison helps establish performance trends and provides useful information for selection of substrates in designing catalytic converter systems. This experimental study tests and compares four ultra thin wall products (400/4, 600/3, 600/4, and 900/2) with a standard wall product (400/6.5) at two different substrate volumes. Engine bench aging is used to simulate typical aged conditions. Temperature data as well as second by second and bag emissions data for hydrocarbons, carbon monoxide and oxides of nitrogen were used to evaluate the relative performances of the substrates. The US FTP and US06 driving cycles were used as protocols for the comparison. Results suggest that lower bulk density and higher geometric surface area interact to lead to lower emissions.
Technical Paper

Ultra Thinwall Light-off Performance - Varying Substrates, Catalysts, and Flow Rates; Models and Engine Testing

2002-03-04
2002-01-0352
To establish performance trends in ultra thin wall substrates and help support their selection criteria for designing catalytic converter systems, the light-off behavior of five Ultra Thin Wall ceramic substrates and two catalysts on an engine dynamometer are hereby examined. Modeling predictions are also compared to the engine results and the trends and implications are discussed. To quantify the performance of these different systems, light-off tests were performed on an engine dynamometer using a simulated FTP cycle. Five systems were evaluated (600/4, 600/3, 600/2, 900/2 and 1200/2) each with two different catalyst formulations. Engine bench aging was used to simulate typical aged conditions in the converter systems. Second by second emissions data for temperature, hydrocarbons and carbon monoxide, were used to evaluate the relative performances of the substrates.
Technical Paper

Evaluation of SoftMountSM Technology for Use in Packaging UltraThinwall Ceramic Substrates

2002-03-04
2002-01-1097
Quantitative in-use pressure measurements were taken from packaging ceramic substrates with the SoftMountSM technology and two more traditional technologies, stuffing and tourniquet. Each technology was assessed using four separate mat materials. Mat selection enhanced the application of the SoftMountSM technology through the reduced pressures applied to the substrate during packaging. High temperature and low temperature thermal cycling studies were performed on the canned converters for the three packaging technologies so that an evaluation could be made of converter durability. The SoftMountSM packaging technology yielded the lowest pressures of all the processes studied, regardless of mat type. The laminar hybrid mat evaluated yielded the best combination of pressure and durability performance. Low temperature residual shear strengths following thermal cycling of the converters showed good correlation between the SoftMountSM technology and the stuffing method.
Technical Paper

The Effect of Environmental Aging on Intumescent Mat Material Durability at Low Temperatures

2002-03-04
2002-01-1099
Mat material durability data in the form of fragility curves were generated in a critical temperature region for three intumescent mat materials considered for low temperature converter applications. The mat materials were tested in a tourniquet wrap converter configuration employing a cylindrical ceramic substrate. Prior to developing durability data for these mat materials, the test items were subjected to various environmental thermal and/or vibration aging conditions. Mat material fragility data were generated in terms of the dynamic force required to impose prescribed differential motion between the can and substrate, thereby, subjecting the mat material to a dynamic shearing like that expected during resonant excitation. As expected, it was found that the mat material capacity to resist shearing deformation decreased when the test samples were subjected to 36 hours of low temperature thermal cyclic aging.
Technical Paper

Shear Strength of Cordierite Ceramic Catalyst Supports

2001-03-05
2001-01-0935
An analytical model for estimating shear and bending stresses during canning of cordierite ceramic catalyst supports is presented. These stresses arise when the radial pressure distribution is nonuniform due, primarily, to variations in gap bulk density (GBD ) of intumescent mat around the perimeter of the substrate. Variations in GBD can occur during canning, regardless of the canning technique, due to anisotropic can stiffness or component tolerances or mat overlap. The model helps relate shear and bending stresses to substrate size and orientation, elastic modulii, cell size and wall porosity. If these stresses approach the corresponding strength of substrate, a shear crack may develop during or after the canning process depending on the magnitude of stress. A special test fixture was developed to measure the shear strength of ceramic catalyst supports, with different cell sizes, before and after the application of washcoat.
Technical Paper

A New High Temperature Ceramic Material for Diesel Particulate Filter Applications

2000-10-16
2000-01-2844
Cordierite-based diesel particulate filters (DPFs) have been in use for heavy duty engine applications for nearly two decades. Recently, passenger car applications for DPFs have begun to appear in Europe due to tightening legislation. While cordierite-based DPFs work well in most applications, it appears that in the passenger car exhaust environment under some uncontrolled regeneration conditions, cracking and melting of the existing cordierite-based DPF products have been reported. The present paper focuses on the development of new, high temperature oxide ceramics for DPF passenger car applications. When designed properly, DPFs made from these new materials do not show cracking or melting under uncontrolled regeneration. The material properties (strength, elastic modulus, coefficient of thermal expansion, etc.) and the filter performance properties (pressure drop, regeneration durability, etc.) have been characterized for DPFs made from these new materials.
Technical Paper

Diesel Emission Control - Last 12 Months in Review

2000-10-16
2000-01-2817
The key diesel emission control papers of the last 12 months have been summarized. In addition, the emerging US and European light-duty and heavy-duty tailpipe regulations are compared. Results are reported on light-duty diesel filtration regeneration systems and experiences, including effects of ash build-up and some recent modeling work. On the heavy-duty side, optimization of SCR catalysts and systems are described, as well as experiences with the first integrated SCR/filter systems, which are already achieving “Euro V” 2008 standards. An update on NOx adsorbers is also provided. The results with new NOx formulations are described, as well as the system performance in a light-duty diesel application.
Technical Paper

Measurement of Biaxial Strength of New vs. Used Windshields

2000-10-03
2000-01-2721
This paper presents the strength data for conventional automotive windshields in both the new and used conditions. More specifically, the biaxial strength of outer surface of curved and symmetrically laminated windshield, measured in biaxial flexure, is reported. The relative contributions of inplane membrane stress, which can be significant for new windshields, and bending stress are quantified with the aid of strain gauge rosettes mounted on both the outer and inner surfaces of windshield. The strength distribution for new and used windshields, based on Weibull distribution function, is found to be multimodal indicating more than one family of surface flaws. Depending on handling damage during manufacturing, assembly and installation processes, the low strength region of new windshields can approach that of used windshields with 50,000+ road miles!
Technical Paper

A New Converter Concept Providing Improved Flow Distribution and Space Utilization

1999-03-01
1999-01-0768
A new converter concept is introduced, which utilizes the additional space in the inlet cone of the converter. An optimized design is obtained by the application of computational fluid dynamics (CFD) and flow distribution measurements, resulting in up to 20% improved flow distribution through the substrate. In addition, the volume of the converter can be increased by approximately 15% using the same space envelope. Durability tests of the converter system have been performed using a thermal cycling test on an engine test bench for 135 hours. No deterioration of the substrate or mounting system occurred. The emissions performance was evaluated on a stationary dynamometer. The impact of the flow distribution on the temperature field and the conversion behavior during light-off and steady state operation were investigated. Under the current testing conditions, no differences in light-off behavior were determined, despite significant differences in the temperature field.
Technical Paper

Fatigue and Performance Data for Advanced Thin Wall Ceramic Catalysts

1998-02-23
980670
With stricter emissions standards, low back pressure requirements, and 100,000 mile durability specifications, ceramic catalysts have undergone significant developments over the past few years. The thrust in the ceramics area has centered on thin-wall structures to minimize back pressure and on high cell density for rapid light-off in close-coupled applications. The thin-wall structures are extruded from low expansion cordierite ceramic with adequate strength and thermal shock resistance equivalent to those of standard cordierite substrate. Examples of thin-wall substrate include 350XT which is extruded from a very low expansion dense cordierite ceramic, and 400/4 and 600/4 cell structures extruded from a low expansion modified cordierite ceramic. This paper will focus on the high fatigue resistance, excellent conversion efficiency, and low back pressure of 350 XT substrates with advanced washcoat system.
Technical Paper

Advances of Durability of Ceramic Converter Systems

1996-10-01
962372
Governing bodies world-wide are setting increasingly tighter emission standards to help improve air quality. US and Californian LEV/ULEV standards are pace setting, European Stage II legislation has just become effective. In Brazil, the upcoming 1997 standards are also demanding for tighter emission control. The monolithic ceramic honeycomb catalytic converter -for more than the past 20 years- has been a reliable key element in the automotive emission control systems. In order to help meet tightened emission regulation as well to satisfy even more stringent durability requirement, an advanced thinwall ceramic Celcor XT has been developed for increased geometric surface area and reduced backpressure. The product properties as well as FTP and ECE emission and durability test results are being described in this paper. Converter system durability is also determined by robust canning and mounting systems. A durable mounting concept, especially for preconverters, is being described.
Technical Paper

Low Back Pressure, High Efficiency Automotive Cabin Air Odor Filters

1996-02-01
960943
Preliminary back pressure and adsorption performance results are reported for two activated carbon honeycomb materials. The carbon impregnated honeycomb (CIH) material is porous ceramic honeycomb with a complete impregnation and coating of activated carbon on all ceramic surfaces. It offers the potential to be a permanent odor filter in that it can be in situ electrically regenerated. It has adsorption performance similar to commercially available layered filters, but has much lower back pressure. The second material is an activated carbon honeycomb (ACH) and is not ceramic-based as is CIH. As such, it has much more activated carbon and superior adsorption performance. The back pressure is low, as with CIH. It has significant potential as a high-performing disposable odor filter.
Technical Paper

Systems Design for Ceramic LFA Substrates for Diesel/Natural Gas Flow- Through Catalysts

1995-02-01
950150
The monolithic, large frontal area (LFA), extruded ceramic substrates for diesel flow-through catalysts offer unique advantages of design versatility, longterm durability, ease of packaging and low Cost [1, 2]*. This paper examines the effect of cell density and cell size on catalyst light-off performance, back pressure, mechanical and thermal durability, and the steady-state catalytic activity. The factors which affect these performance characteristics are discussed. Certain trade-offs in performance parameters, which are necessary for optimum systems design, are also discussed. Following a brief discussion of design methodology, substrate selection, substrate/washcoat interaction and packaging specifications, the durability data for ceramic flow-through catalysts are summarized. A total of over 18 million vehicle miles have been successfully demonstrated by ceramic LFA catalysts using the systems design approach.
Technical Paper

Durability of Extruded Electrically Heated Catalysts

1995-02-01
950404
Extruded metal honeycombs are used as electrically heated catalysts (EHCs). The durability requirements of this application make demands on high surface area, thin cross-section metal honeycombs. Significant durability improvements over previous extruded metal honeycomb EHCs have been achieved by material and package design changes. The product redesign was supported by finite element models and extensive testing. The redesigned EHC has passed severe laboratory and field testing. The tests include electrical cycling to 1000°C/1600 cycles, hot vibration to 60g/900°C and demanding on-vehicle exposure. Excellent durability of the extruded metal honeycomb has been demonstrated.
Technical Paper

High Temperature Compressive Strength of Extruded Cordierite Ceramic Substrates

1995-02-01
950787
High temperature modulus of rupture (MOR) data, published previously, show that the ceramic catalyst supports get stronger with temperature due to the absence of water vapor and closure of microcracks which would otherwise act as stress concentrators [1, 2 and 3]*. The increased MOR value is partially responsible for the excellent durability of ceramic catalyst supports at high temperature. In this paper, we will present the compressive strength data of ceramic substrates at high temperature, namely the crush strength along B-axis and biaxial compressive strength of the whole substrate. Since the honeycomb strength is directly related to that of the individual cell wall, the compressive strength should also increase with temperature similar to the modulus of rupture. Accordingly, the ceramic substrates are capable of supporting higher mounting pressures exerted by the intumescent mat at high temperature [4].
Technical Paper

Design Considerations for a Ceramic Preconverter System

1994-03-01
940744
The preconverter is an essential element of exhaust gas treatment to help meet the tighter emission standards of TLEV and LEV levels. Its design must be chosen so as to meet the simultaneous requirements of compactness, faster light-off, low back pressure, high temperature durability and low cost. This paper presents design options for a ceramic substrate and durable package which lead to an optimum and cost-effective preconverter system. Preliminary data for high temperature physical durability of selected converter systems are presented. Performance parameters for light-off activity and back pressure are also computed and compared with those of standard substrates used in underbody application. Laboratory tests comprising of axial push-out test, high temperature vibration test, exhaust gas simulation test and the engine dynamometer test demonstrate the viability of ceramic preconverters for automotive application.
Technical Paper

High Temperature Durability of Electrically Heated Extruded Metal Support

1994-03-01
940782
The design, performance and optimization of the extruded electrically heated metal converter have recently been published(1,2). The present paper focuses on the physical durability of extruded metal EHC support at high temperature representative of operating conditions. The mechanical, thermal, creep and fatigue properties of Fe-Cr-Al honeycomb structure over 25°-1000°C temperature range are reported. In addition, the stresses arising from mounting and thermal loads are computed via finite element analysis and compared with the high temperature strength of extruded metal EHC support. A safe design stress which predicts 192,000 kilometer durability is estimated from high temperature fatigue behavior of extruded Fe-Cr-Al honeycomb structure.
Technical Paper

Effect of Contour, Size and Cell Structure on Compressive Strength of Porous Cordierite Ceramic Substrates

1993-10-01
932663
Since their introduction to automotive industry in 1975, ceramic substrates have successfully met the strength requirements for canning, engine and chassis vibrations, and thermal shock. This paper will focus on canning loads and techniques, and how they influence the stress distribution in ceramic substrates. The strength data, most relevant to canning stresses, will be presented for porous cordierite ceramic substrates as function of their contour, size and cell structure. Recent improvements in measuring the biaxial compressive strength will also be reviewed.