Journal Article

A Study on Flexible Transparent Electrode Materials for Touch Sensor

2023-04-11
2023-01-0074
As the AVN display in the car interior becomes larger and located above the center fascia, the driver's visual visibility is becoming important. In addition, since an expensive touch sensor is installed, a transparent electrode cost reduction technology for a display touch sensor that can replace an indium material, which is an expensive rare metal, is required. In this paper, we developed new transparent electrode materials and manufacturing methods for the touch sensor film which light reflectance is low and flexible without a separate low-reflection multi-layer, so that the design freedom is high and the material cost is low. By optimizing the amount of fluorine doping ratio in tin oxide, excellent electrical conductivity and high optical transmittance are secured, and the surface reflectance is reduced by adjusting the diameter and length of the silver nanowire. As a result, it was shown that the AVN display image and font readability was improved.
Technical Paper

Development of Surfactant-Free Anti-Fogging Coating for Automotive Headlamps

2019-03-25
2019-01-1439
Recently, the design of automotive headlamps has become diversified and complicated according to customer needs. Hence, structural complexity of the headlamps has also increased. Complex structure of the headlamps inevitably causes a disturbance in air circulation. For this reason, inadvertent micro-sized water droplets, called fogging, are condensed on the inner surface of headlamp lens due to temperature difference between the inner and outer lens surfaces. To circumvent fogging inside of the headlamp lens, an anti-fogging coating is indispensable. Conventionally, diverse surfactants have been adopted as substantial material for the anti-fogging coating. However, the usage of the surfactants causes undesirable side effect such as water mark arising from vapor condensation, which is an important issue that must be fully resolved. In this study, we developed an innovative anti-fogging coating material without using conventional surfactant.
Technical Paper

Microstructure and Tribological Behavior of CrN-Cu Nanocoatings Deposited by PVD Systems

2016-04-05
2016-01-0492
The present study focused on CrN-Cu nanocoatings composed of nano-meter grains with CrN, Cr and Cu functioning low-friction, anti-wear and heat resistance. The coatings were synthesized by hybrid PVD including metal arc source, magentron sputter source and ion-gun source. Although Cu has low hardness, the hardness of CrNCu is not declined because it was composed of below 20nm sized grains of CrN, Cr, and Cu. However, CrN-Cu had lower friction than CrN owing to Cu’s low shear strength. CrN-Cu films optimized using the Reaction Surface Method (RSM) showed the excellent tribological behavior and low coefficient of friction compared with DLC. The tribological properties of the Cr-Cu-N demonstrated superior wear resistance and low friction at normal and high temperature conditions. The CrN-Cu nanocoatings can be used for the downsizing automotive engines working at severe tribological conditions.
Technical Paper

Development of Si-DLC Coated Tappet for Improved Wear Resistance

2015-04-14
2015-01-0685
Most bucket type valvetrain engines use DLC coated tappet for low friction and fuel efficiency. However the requirements on coating robustness have been increased as the tribological environments have become more severe by use of low viscosity oil or higher engine output. In order to obtain higher coating efficiency and improved wear resistance, 5∼9 at.% Si doped DLC (Si-DLC) coated tappet has been developed using PACVD process. Thermal stability and wear resistance of Si-DLC were improved impressively than those of DLC, although mechanical properties such as hardness and adhesion were degradated. It seems that Si suppresses a graphitization of DLC and thin SixOy film on coating surface acts as a barrier to oxidation or flash heat.
Journal Article

Development of Nano Diamond Polymer Coating on Piston Skirt for Fuel Efficiency

2011-04-12
2011-01-1401
Various polymer-based coatings are applied on piston skirt to reduce friction loss between the piston skirt and cylinder bore which is one of main factors of energy loss in an automotive engine system. These coatings generally consist of polymer binder (PAI) and solid lubricants (graphite or MoS₂) for low friction property. On the other hand, the present study found that PTFE as a solid lubricant and nano diamond as hard particles can be used to improve the low friction and wear resistance simultaneously. In the process of producing coating material, diamond particles pulverized to a nano size tend to agglomerate. To prevent this, silane (silicon coupling agent) treatment was applied. The inorganic functional groups of silane are attached to the nano diamond surface, which keep the diamond particles are apart.
Technical Paper

Development of Engine Control Using the In-Cylinder Pressure Signal in a High Speed Direct Injection Diesel Engine

2011-04-12
2011-01-1418
Emissions regulations are becoming more severe, and they remain a principal issue for vehicle manufacturers. Many engine subsystems and control technologies have been introduced to meet the demands of these regulations. For diesel engines, combustion control is one of the most effective approaches to reducing not only engine exhaust emissions but also cylinder-by-cylinder variation. However, the high cost of the pressure sensor and the complex engine head design for the extra equipment are stressful for the manufacturers. In this paper, a cylinder-pressure-based engine control logic is introduced for a multi-cylinder high speed direct injection (HSDI) diesel engine. The time for 50% of the mass fraction to burn (MFB50) and the IMEP are valuable for identifying combustion status. These two in-cylinder quantities are measured and applied to the engine control logic.
Technical Paper

Development of High Wear Resistant and Durable Coatings for Al Valve Spring Retainer

2007-04-16
2007-01-1748
The use of light-weight materials in automotive engine components has increased in order to achieve better fuel efficiency and engine performance. In this study, Al alloy (AI5056) valve spring retainer can reduce a weight by 63% in comparison to steel and improve the upper limit of engine speed by about 500rpm. The Al valve spring retainer was fabricated by cold forging and coated with hard anodizing, DLC (diamond like coating), cold spray and thermal spray for better wear resistance and durability. We conclude that among these materials the DLC coating improves the wear resistance of Al valve spring retainer and has a sufficient durability after endurance testing.