Refine Your Search

Topic

Search Results

Standard

COATING, ALUMINUM OXIDE Detonation Deposition

1993-10-01
HISTORICAL
AMS2436C
This specification covers the engineering requirements for applying aluminum oxide to metal parts by detonation deposition and the properties of such coatings.
Standard

Coating, Tungsten Carbide-Cobalt Detonation Process

2001-04-01
HISTORICAL
AMS2435F
This specification covers the engineering requirements for applying tungsten carbide/cobalt coatings to metal parts by the detonation process and the properties of such coatings.
Standard

TUNGSTEN CARBIDE-COBALT COATING Detonation Process

1994-10-01
HISTORICAL
AMS2435E
This specification covers the engineering requirements for applying tungsten carbide/cobalt coatings to metal parts by the detonation process and the properties of such coatings.
Standard

PEENING MEDIA Cast Steel Shot, Regular (45 - 52 HRC)

1994-04-01
HISTORICAL
AMS2431/1
This specification, in conjunction with the general requirements covered in AMS 2431, establishes the requirements for regular cast steel shot to be used for peening of metal parts.