Standard Steel Tubing (Seamless for Machined Parts) 1.8ni 0.80cr 0.25mo (0.38 - 0.43c) Heat Treated (200,000 Tensile Strength) 2002-12-16 CURRENT AMS6420
Standard STEEL TUBING (WELDED) Chromium Molybdenum (.27 - .33 Carbon) (Normalized) 1942-06-01 HISTORICAL AMS6510
Standard Steel Tubing (Seamless for Machined Parts) .55ni .25mo (.33 - .38c) Normalized Or Heat-Treated (90,000 Tensile Strength) 2002-12-16 CURRENT AMS6283
Standard Steel Tubing (Seamless for Machined Parts) .55ni .50cr .25mo (.35 - .38c) Heat-Treated (125,000 Tensile Strength) 2002-12-16 CURRENT AMS6284
Standard Steel Tubing (Seamless for Machined Parts) .55ni .50cr .25mo (.38 - .43c) Heat-Treated (180,000 Tensile Strength) 2002-12-16 CURRENT AMS6285
Standard Steel Tubing (Seamless for Machined Parts) .55ni .50cr .25mo (.38-.43c) Heat-Treated (180,000 T.S.) 2002-12-16 CURRENT AMS6286
Standard NUTS, SELF-LOCKING, STEEL High Strength, Prevailing-Torque, All Metal 450 F (232 C) Use, Unified "J" (MIL-S-8879) Thread Form 1969-11-01 HISTORICAL AMS7252
Standard NUTS, SELF-LOCKING, STEEL High Strength, All Metal 450° F (230° C) Use, Unified "J" (MIL-S-8879) Thread Form 1980-01-15 HISTORICAL AMS7252B This specification covers all-metal, self-locking nuts, plate nuts, and gang channel nuts made of a carbon or low-alloy steel.
Standard NUTS, SELF-LOCKING, STEEL High Strength, Prevailing Torque, All Metal 450° F (232° C) Use, Unified "J" (MIL-S-8879) Thread Form 1973-05-15 HISTORICAL AMS7252A This specification covers all-metal, self-locking, prevailing-torque nuts, plate nuts, and gang channel nuts made of a carbon or low-alloy steel.
Standard Forgings, Hardenable Steels and Corrosion-Resistant Steels Heat-Treated, Finished-Part Properties Short-Transverse Tensile Strength and Fracture Toughness 2012-10-03 HISTORICAL AMS6474A This specification establishes requirements for steel forgings of any shape or form that finished parts are to be made (See 8.4, 8.5, 8.8.4 and 8.10).
Standard DUCTILE (NODULAR) IRON CASTINGS, SAND 60,000 psi (415 MPa) Tensile Strength Ferritize Annealed 2011-08-10 HISTORICAL AMS5315C This specification covers a ductile (nodular) iron in the form of sand castings.
Standard Ductile (Nodular) Iron Castings, Sand 60,000 psi (415 MPa) Tensile Strength Ferritize Annealed 2013-04-03 HISTORICAL AMS5315D This specification covers a ductile (nodular) iron in the form of sand castings.
Standard DUCTILE (NODULAR) IRON CASTINGS, SAND 60,000 psi (414 MPa) Tensile Strength 1981-07-01 HISTORICAL AMS5315B This specification covers a ductile (nodular) iron in the form of sand castings.