The Influence of Ammonia Slip Catalysts on Ammonia, N2O and NOX Emissions for Diesel Engines

2007-04-16
2007-01-1572
The use of urea-based selective catalytic reduction (SCR) is a promising method for achieving U.S. Tier 2 diesel emission standards for NOx. To meet the Tier 2 standards for Particulate Matter (PM), a catalyzed diesel particulate filter (CDPF) will likely be present and any ammonia (NH3) that is not consumed over an SCR catalyst would pass over the CDPF to make nitrous oxide (N2O) emissions and/or oxides of nitrogen (NOx), or exit the exhaust system as NH3. N2O is undesirable due to its high greenhouse gas potential, while NOx production from the slipped NH3 would reduce overall system NOx conversion efficiency. This paper reviews certain conditions where NH3 slip past an SCR system may be a concern, looks at what would happen to this slipped NH3 over a CDPF, and evaluates the performance of various supplier NH3 slip catalysts under varied space velocities, temperatures and concentrations of NH3 and NOx.
Technical Paper

The Effects of SO2 and SO3 Poisoning on Cu/Zeolite SCR Catalysts

2009-04-20
2009-01-0898
Copper/zeolite catalysts are the leading urea SCR catalysts for NOx emission treatment in diesel applications. Sulfur poisoning directly impacts the overall SCR performance and is still a durability issue for Cu/zeolite SCR catalysts. Most studies on sulfur poisoning of Cu/zeolite SCR catalysts have been based on SO2 as the poisoning agent. It is important to investigate the relative poisoning effects of SO3, especially for systems with DOCs in front of Cu/zeolite SCR catalysts. It was observed that SCR activity was significantly reduced for samples poisoned by SO3 vs. those poisoned by SO2. The sulfur was released mainly as SO2 for both samples poisoned by SO2 and SO3. The temperatures and the magnitudes of released SO2 peaks however, were very different between the samples poisoned by SO2 vs. SO3. The results indicate that sulfur poisoning by SO2 and SO3 are not equivalent, with different poisoning mechanisms and impacts.
Journal Article

Sulfur Tolerance and DeSOx Studies on Diesel SCR Catalysts

2008-04-14
2008-01-1023
Base metal/zeolite catalysts, particularly containing copper and iron, are among the leading candidates for treatment of NOx emissions for diesel applications. Even with the use of ultra low sulfur fuel, sulfur poisoning is still a durability issue for base metal/zeolite SCR catalysts. In this study, the impact of sulfur poisoning on SCR activity and the stored sulfur removal effectiveness were investigated on several Cu and Fe/zeolite SCR catalysts after different thermal aging. The impact of sulfur was more significant on the Cu than on Fe/zeolite SCR catalysts for the NOx activity. It was found that the sensitivity of thermal aging status to the sulfur poisoning impact was different. The impact of sulfur on NOx activity changed with thermal aging on some catalysts, while it remained relatively the same for other catalysts. The most thermally durable SCR catalyst was not necessarily the most durable to sulfur poisoning.
Journal Article

Soot and Ash Deposition Characteristics at the Catalyst-Substrate Interface and Intra-Layer Interactions in Aged Diesel Particulate Filters Illustrated using Focused Ion Beam (FIB) Milling

2012-04-16
2012-01-0836
The accumulation of soot and lubrication-derived ash particles in a diesel particulate filter (DPF) increases exhaust flow restriction and negatively impacts engine efficiency. Previous studies have described the macroscopic phenomenon and general effects of soot and ash accumulation on filter pressure drop. In order to enhance the fundamental understanding, this study utilized a novel apparatus that of a dual beam scanning electron microscope (SEM) and focused ion beam (FIB), to investigate microscopic details of soot and ash accumulation in the DPF. Specifically, FIB provides a minimally invasive technique to analyze the interactions between the soot, ash, catalyst/washcoat, and DPF substrate with a high degree of measurement resolution. The FIB utilizes a gallium liquid metal ion source which produces Ga+ ions of sufficient momentum to directionally mill away material from the soot, ash, and substrate layers on a nm-μm scale.
Journal Article

Post Mortem of an Aged Tier 2 Light-Duty Diesel Truck Aftertreatment System

2009-11-02
2009-01-2711
A 2005 prototype diesel aftertreatment system consisting of diesel oxidation catalysts (DOC), Cu/zeolite Selective Catalytic Reduction (SCR) catalyst, and Catalyzed Diesel Particulate Filter (CDPF) was aged to an equivalent of 120k mi on an engine dynamometer using an aging cycle that incorporated both city and highway driving modes. The program demonstrated durable reduction in particulate matter (PM) and nitrogen oxides (NOx) emissions to federal Tier 2 levels on a 6000 lbs light-duty truck application. Very low sulfur diesel fuel (∼15 ppm) enabled lower PM emissions, reduced the fuel penalty associated with the emission control system, and improved long-term system durability. A total of 643 filter regenerations occurred during the aging that raised the entire catalyst system to high temperatures on a regular basis. After testing the aged system on a 6000 lbs light-duty diesel truck, a post mortem analysis was completed on core samples taken from the DOC, SCR catalyst, and filter.
Technical Paper

Phenomenological Investigations of Mid-Channel Ash Deposit Formation and Characteristics in Diesel Particulate Filters

2019-04-02
2019-01-0973
Accumulation of lubricant and fuel derived ash in the diesel particulate filter (DPF) during vehicle operation results in a significant increase of pressure drop across the after-treatment system leading to loss of fuel economy and reduced soot storage capacity over time. Under certain operating conditions, the accumulated ash and/or soot cake layer can collapse resulting in ash deposits upstream from the typical ash plug section, henceforth termed mid-channel ash deposits. In addition, ash particles can bond (either physically or chemically) with neighboring particles resulting in formation of bridges across the channels that effectively block access to the remainder of the channel for the incoming exhaust gas stream. This phenomenon creates serious long-term durability issues for the DPF, which often must be replaced. Mid-channel deposits and ash bridges are extremely difficult to remove from the channels as they often sinter to the substrate.
Technical Paper

Modeling Study of Urea SCR Catalyst Aging Characteristics

2007-04-16
2007-01-1580
This paper presents a study of urea SCR catalyst aging characteristics and implementation into an analytical model that complements laboratory based experiments for a dynamometer-aged SCR brick. The model calibration is based on measured data taken from a 120k-mile simulated dynamometer-aged base metal/zeolite SCR. Dynamometer aging led to non-uniform axial deterioration with more severe deactivation toward the front of the SCR brick compared to the rear. Data from a 120k-mile simulated hydrothermally oven-aged SCR (uniform axial aging) is used to establish baseline aged NOx performance and NH3 adsorption/desorption behavior. An axial deterioration factor is applied to the baseline model to account for differences between oven and dynamometer aging. The model is exercised using engine out vehicle data to examine how different aging processes (oven vs. dynamometer) affect overall NOx performance during the EPA FTP (Environmental Protection Agency Federal Test Procedure).
Journal Article

Lubricant-Derived Ash Impact on Gasoline Particulate Filter Performance

2016-04-05
2016-01-0942
The increasing use of gasoline direct injection (GDI) engines coupled with the implementation of new particulate matter (PM) and particle number (PN) emissions regulations requires new emissions control strategies. Gasoline particulate filters (GPFs) present one approach to reduce particle emissions. Although primarily composed of combustible material which may be removed through oxidation, particle also contains incombustible components or ash. Over the service life of the filter the accumulation of ash causes an increase in exhaust backpressure, and limits the useful life of the GPF. This study utilized an accelerated aging system to generate elevated ash levels by injecting lubricant oil with the gasoline fuel into a burner system. GPFs were aged to a series of levels representing filter life up to 150,000 miles (240,000 km). The impact of ash on the filter pressure drop and on its sensitivity to soot accumulation was investigated at specific ash levels.
Technical Paper

Laboratory Testing of Urea-SCR Formulations to Meet Tier 2 Bin 5 Emissions

2007-04-16
2007-01-1575
Urea-based Selective Catalytic Reduction (SCR) has the potential to meet U.S. Diesel Tier 2 Bin 5 emission standards for NOx in 2010. The operating and driving conditions of light-duty and heavy-duty vehicles make it necessary to customize catalyst features to the application. This paper reviews the selection of SCR catalyst technology for the U.S. and the appropriate aging and poisoning protocols for current supplier SCR catalysts. Generally, light-duty applications require SCR catalysts to function well at low temperature whereas heavy-duty applications require functionality at high temperature and high space velocity. One main durability requirement of SCR formulations involves withstanding the high temperature process of regenerating particulate filters from accumulated soot. Unrefined engine exhaust temperature control coupled with the inexact temperature measurement may also expose SCR catalysts to additional over-temperature conditions.
Journal Article

Laboratory Study of Soot, Propylene, and Diesel Fuel Impact on Zeolite-Based SCR Filter Catalysts

2009-04-20
2009-01-0903
Selective Catalytic Reduction (SCR) catalysts have been designed to reduce NOx with the assistance of an ammonia-based reductant. Diesel Particulate Filters (DPF) have been designed to trap and eventually oxidize particulate matter (PM). Combining the SCR function within the wall of a high porosity particulate filter substrate has the potential to reduce the overall complexity of the aftertreatment system while maintaining the required NOx and PM performance. The concept, termed Selective Catalytic Reduction Filter (SCRF) was studied using a synthetic gas bench to determine the NOx conversion robustness from soot, coke, and hydrocarbon deposition. Soot deposition, coke derived from propylene exposure, and coke derived from diesel fuel exposure negatively affected the NOx conversion. The type of soot and/or coke responsible for the inhibited NOx conversion did not contribute to the SCRF backpressure.
Technical Paper

Laboratory Studies and Mathematical Modeling of Urea SCR Catalyst Performance

2007-04-16
2007-01-1573
This paper presents the development of an analytical model that complements laboratory based experiments to provide a tool for Selective Catalyst Reduction (SCR) applications. The model calibration is based on measured data from NOx reduction performance tests as well as ammonia (NH3) adsorption/desorption tests over select SCR catalyst formulations in a laboratory flow reactor. Only base metal/zeolite SCR samples were evaluated. Limited validations are presented that show the model agrees well with vehicle data from Environmental Protection Agency Federal Test Procedure (EPA FTP) emission assessments. The model includes energy and mass balances, several different NH3 reactions with NOx, NH3 adsorption and desorption algorithms, and NH3 oxidation.
Technical Paper

Laboratory Postmortem Analysis of 120k mi Engine Aged Urea SCR Catalyst

2007-04-16
2007-01-1579
Selective Catalytic Reduction (SCR) of NOx with aqueous urea and a Catalyzed Diesel Particulate Filter (CDPF) has been considered as one of the emission control systems for diesel vehicles required to meet Federal Tier 2 and California LEVII emission standards. At Ford Motor Company, a DOC-SCR-CDPF system containing a copper / zeolite SCR catalyst was aged to 120k mi on the engine dynamometer using an aging cycle that mimicked both city and highway driving modes. A total of 643 CDPF regenerations occurred during the aging that raised the SCR catalyst to a temperature of up to 650°C on a regular basis. A series of lab analyses including activity tests, ammonia thermal desorption, BET surface area, XRF, XRD, and EPMA was conducted on cores taken from the 120k mi engine aged SCR catalyst brick. The lab post-mortem characterizations revealed the changes of catalyst properties, and the deterioration profile of the SCR catalyst brick after undergoing real aging conditions.
Journal Article

Impact and Prevention of Ultra-Low Contamination of Platinum Group Metals on SCR Catalysts Due to DOC Design

2009-04-20
2009-01-0627
Diesel aftertreatment systems configured with a diesel oxidation catalyst (DOC) upstream of an urea selective catalytic reduction (SCR) catalyst run the risk of precious metal contamination. During active diesel particulate filter (DPF) regeneration events, the DOC bed temperature can reach up to 850°C. Under these conditions, precious metal (especially Pt) can be volatized and then deposited on a downstream SCR catalyst. In this paper, the impact of ultra-low contamination of platinum group metals (PGM) on the SCR catalyst was studied. A method based on precious metal volatilization of a Pt-rich DOC at 850°C and under lean gas conditions was employed to contaminate downstream FeSCR and CuSCR formulations. The contamination resulted in poor NOx conversion (via NOx remake) and excessive N2O formation. The precious metal volatilization method was employed to screen various Pt/Pd based DOCs to avoid contamination of the downstream FeSCR.
Technical Paper

Factors Affecting Diesel LNT Durability in Lab Reactor Studies

2004-03-08
2004-01-0156
Promising lean NOx trap (LNT) results on lean-burn gasoline engines have encouraged the development of LNTs for diesel applications. Although the fundamentals of LNT are common for both gasoline and diesel applications, there are major differences due to the character of engine operation and control strategies. The sulfur tolerance and thermal durability of current state-of-the-art diesel LNTs under the conditions that represent the thermal and chemical conditions in diesel exhaust were investigated in a laboratory flow reactor. Sulfur poisoning and thermal aging are unavoidable factors contributing to diesel LNT deactivation. The results show that sensitivity to sulfur poisoning varies with the catalyst formulations, and in some formulations the sulfur poisoning appears reversible. However, the thermal deactivation is permanent regardless of its cause, i.e., LNT de-sulfation (deSOx) or diesel particular filter (DPF) regeneration.
Journal Article

Enhanced Durability of a Cu/Zeolite Based SCR Catalyst

2008-04-14
2008-01-1025
Passenger and light duty diesel vehicles will require up to 90% NOx conversion over the Federal Test Procedure (FTP) to meet future Tier 2 Bin 5 standards. This accomplishment is especially challenging for low exhaust temperature applications that mostly operate in the 200 - 350°C temperature regime. Selective catalytic reduction (SCR) catalysts formulated with Cu/zeolites have shown the potential to deliver this level of performance fresh, but their performance can easily deteriorate over time as a result of high temperature thermal deactivation. These high temperature SCR deactivation modes are unavoidable due to the requirements necessary to actively regenerate diesel particulate filters and purge SCRs from sulfur and hydrocarbon contamination. Careful vehicle temperature control of these events is necessary to prevent unintentional thermal damage but not always possible. As a result, there is a need to develop thermally robust SCR catalysts.
Journal Article

Direct Measurements of Soot/Ash Affinity in the Diesel Particulate Filter by Atomic Force Microscopy and Implications for Ash Accumulation and DPF Degradation

2014-04-01
2014-01-1486
Inorganic engine lubricant additives, which have various specific, necessary functions such as anti-wear, leave the combustion chamber bound to soot particles (approximately ≤1% by mass) as ash [13], and accumulate in aftertreatment components. The diesel particulate filter (DPF) is especially susceptible to ash-related issues due to its wall-flow architecture which physically traps most of the soot and ash emissions. Accumulated lubricant-derived ash results in numerous problems including increased filter pressure drop and decreased catalytic functionality. While much progress has been made to understand the macroscopic details and effects of ash accumulation on DPF performance, this study explores the nano- and micron-scale forces which impact particle adhesion and mobility within the particulate filter.
Technical Paper

Development of Emission Transfer Functions for Predicting the Deterioration of a Cu-Zeolite SCR Catalyst

2009-04-20
2009-01-1282
Urea selective catalytic reduction (SCR) catalysts have the capability to deliver the high NOx conversion efficiencies required for future emission standards. However, the potential for the occasional over-temperature can lead to the irreversible deactivation of the SCR catalyst. On-board diagnostics (OBD) compliance requires monitoring of the SCR function to make sure it is operating properly. Initially, SCR catalyst performance metrics such as NOx conversion, NH3 oxidation, NH3 storage capacity, and BET surface area are within normal limits. However, these features degrade with high temperature aging. In this work, a laboratory flow reactor was utilized to determine the impact on these performance metrics as a function of aging condition. Upon the completion of a full time-at-temperature durability study, four performance criteria were established to help determine a likely SCR failure.
Technical Paper

Deactivation of Cu/Zeolite SCR Catalyst under Lean-Rich Aging Conditions

2010-04-12
2010-01-1180
A lean-rich hydrothermal aging was used to study the deactivation of Cu-zeolite SCR catalyst that has enhanced stability. Impact of DOC upstream on the SCR catalyst during the lean-rich aging was also investigated. The LR hydrothermal aging was conducted with the presence of hydrocarbon, CO and H₂ at different O₂ levels. It was found that the SCR catalyst was active for the oxidation of CO, H₂ and hydrocarbon, resulting in significant exotherm across the catalyst. In addition to hydrothermal aging, reductive aging, especially the presence of H₂ in the aging gas stream without O₂ presence during the L-R aging, might also contribute to the Cu/zeolite SCR catalyst deactivation. The impacts of DOC upstream on Cu/zeolite SCR catalysts depended on the aging temperatures. At lower aging temperature, the uncompleted oxidation of hydrocarbon and CO on the DOC might cause steam reforming and water-gas shift reactions on the DOC to form reductive gas stream.
Journal Article

Deactivation of Cu/Zeolite SCR Catalyst Due To Reductive Hydrothermal Aging

2008-04-14
2008-01-1021
Temperature programmed reduction by CO, H2, and propylene (C3H6), as well as hydrothermal aging in the presence of mixture of NO, HC, CO, H2 and O2 were used to study the deactivation of Cu/zeolite SCR catalysts. The presence of CO had no detrimental effect on catalyst activity. Carbonaceous deposit on the catalyst surface from propylene (C3H6) reduction suppressed the catalyst activity and burn off of carbonaceous deposit recovered activity, the presence of O2 suppressed carbonaceous deposit formation. The presence of H2 under lean conditions had much less effect on catalyst activity than H2 presence under rich conditions. Rich conditions with O2 presence represented the most detrimental effect on catalyst activity.
Technical Paper

Cu/Zeolite SCR on High Porosity Filters: Laboratory and Engine Performance Evaluations

2009-04-20
2009-01-0897
Selective catalytic reduction (SCR) is expected to be used extensively in the U.S. for diesel vehicle NOx control. Much progress has been made on improving performance and reducing complexity of SCR systems for vehicles in the past several years. SCR system complexity can be reduced further by implementation of SCR-coated diesel particulate filters (SCRFs). In this system, a high porosity (> 50%) filter substrate is coated with an SCR formulation, ideally in the pores of the filter walls, so that the DPF and SCR functions can be combined into a single catalyst. Two state-of-the-art Cu/zeolite SCR formulations and three types of high porosity filter substrates were included in this study. Laboratory and engine-dynamometer tests were performed to measure NOx conversion under a variety of conditions to assess the impact of ammonia oxidation, inlet NO2/NOx ratio, ammonia/NOx ratio, oxygen level, space velocity, soot loading, and ammonia loading level.
X