Standard

CAST STEEL GRIT

1993-03-01
J1993_199303
This SAE Recommended Practice describes the chemical composition and the physical requirements for high carbon cast steel grit.
Standard

SAE MANUAL ON BLAST CLEANING

1968-06-01
J792A_196806
Blast cleaning may be defined as a secondary manufacturing process in which a suitable stream of solid particles is propelled with sufficient velocity against a work surface to cause a cleaning or abrading action when it comes in contact with the workpiece. As indicated in the definition, blast cleaning may be employed for a variety of purposes. Ordinarily, it is considered as a method for removing sand from castings, burrs or scale from forgings, mill products, or heat treated parts; to promote machinability, and to minimize the possibility of interference in actual operation. In addition to this use, blast cleaning also produces an excellent surface for industrial coatings. All these objectives are often accomplished in the one operation.
Standard

SAE Manual on Blast Cleaning

2022-09-23
J792_202209
Blast cleaning may be defined as a mechanical pre-treatment process in which a suitable stream of solid particles is propelled with sufficient velocity against a work surface to cause a cleaning or abrading action when it comes in contact with the workpiece. Blast cleaning may be employed for a variety of purposes. It is a well-established method for removing sand from castings and burrs or scale from forgings, mill products, or heat treated parts; to promote machinability; and to minimize the possibility of interference in actual operation. In addition to this use, blast cleaning also produces a suitable surface for downstream industrial coatings. All these objectives are often accomplished in the one operation. As a general understanding, this document pertains to blast cleaning only. Any reference to shot peening or other processes is only to explain a context or concept related to blast cleaning.
Standard

SPECIFICATIONS FOR LOW CARBON CAST STEEL SHOT

1991-06-01
J2175_199106
This SAE Recommended Practice describes chemical analysis, hardness, microstructure, and physical characteristic requirements for low carbon cast steel shot to be used for shot peening or blast cleaning operations.
Standard

Shot Peening

2015-06-30
J2441_201506
This SAE Standard covers the engineering requirements for peening surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot.
Standard

Shot Peening

2000-08-01
J2441_200008
This SAE Standard covers the engineering requirements for peening surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot.
Standard

Shot Peening

2021-10-17
WIP
J2441
This SAE Standard covers the engineering requirements for peening surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot. To induce residual compressive stress in surface layers of parts, thereby increasing fatigue strength and resistance to stress-corrosion cracking.
Standard

Specifications for Low Carbon Cast Steel Shot

2021-07-07
J2175_202107
This SAE Recommended Practice describes chemical analysis, hardness, microstructure, and physical characteristic requirements for low carbon cast steel shot to be used for shot peening or blast cleaning operations.
Standard

Specifications for Low Carbon Cast Steel Shot

2015-06-18
J2175_201506
This SAE Recommended Practice describes chemical analysis, hardness, microstructure, and physical characteristic requirements for low carbon cast steel shot to be used for shot peening or blast cleaning operations.