Automotive Austempered Ductile (Nodular) Iron Castings (ADI)

2018-01-09
J2477_201801
This SAE Standard covers the mechanical and physical property requirements for Austempered Ductile Iron (ADI) castings used in automotive and allied industries. Specifically covered are: a Hardness b Tensile Strength c Yield Strength d Elongation e Modulus of Elasticity f Impact Energy g Microstructure In this document SI units are primary and in-lb units are derived. Appendix A provides general information and related resources on the microstructural, chemical and heat treatment requirements to meet the mechanical properties needed for ADI in particular service conditions and applications.
Standard

Automotive Austempered Ductile (Nodular) Iron Castings (ADI)

2004-05-26
J2477_200405
This SAE Standard covers the mechanical and physical property requirements for Austempered Ductile Iron (ADI) castings used in automotive and allied industries. Specifically covered are: a Hardness b Tensile Strength c Yield Strength d Elongation e Modulus of Elasticity f Impact Energy g Microstructure In this document SI units are primary and in-lb units are derived. Appendix A provides general information and related resources on the microstructural, chemical and heat treatment requirements to meet the mechanical properties needed for ADI in particular service conditions and applications.
Standard

Automotive Compacted Graphite Iron Castings

2007-12-17
J1887_200712
This SAE Standard covers the mechanical and physical requirements for Compacted Graphite Iron (CGI) castings used in automotive and allied industries. Requirements in this document include: a Tensile Strength b Yield Strength c Elongation d Graphite Morphology
Standard

Automotive Compacted Graphite Iron Castings

2018-02-15
J1887_201802
This SAE Standard covers the mechanical and physical requirements for Compacted Graphite Iron (CGI) castings used in automotive and allied industries. Requirements in this document include: a Tensile Strength b Yield Strength c Elongation d Graphite Morphology
Standard

Automotive Ductile (Nodular) Iron Castings

2017-12-20
J434_201712
This SAE standard covers the minimum mechanical properties measured on separately cast test pieces of varying thickness and microstructural requirements for ductile iron castings used in automotive and allied industries. Castings may be specified in the as-cast or heat-treated condition. If castings are heat-treated, prior approval from the customer is required. The appendix provides general information on chemical composition, microstructure and casting mechanical properties, as well as other information for particular service conditions. In this standard SI units are primary and in-lb units are derived.
Standard

Automotive Ductile (Nodular) Iron Castings

2004-02-17
J434_200402
This SAE standard covers the minimum mechanical properties measured on separately cast test pieces of varying thickness and microstructural requirements for ductile iron castings used in automotive and allied industries. Castings may be specified in the as-cast or heat-treated condition. If castings are heat-treated, prior approval from the customer is required. The appendix provides general information on chemical composition, microstructure and casting mechanical properties, as well as other information for particular service conditions. In this standard SI units are primary and in-lb units are derived.
Standard

CLASSIFICATION OF COMMON IMPERFECTIONS IN SHEET STEEL

1996-03-01
J810_199603
Common or obvious surface imperfections, which sometimes occur in sheet steel, are normally visible to the naked eye before or after fabrication. Illustrations and definitions of these imperfections are contained in this SAE Information Report. The identifying names are those commonly used throughout the steel industry. The imperfections identified include the major and most often encountered imperfections known to exist at this time. These imperfections are variable in appearance and severity. Extreme conditions have been selected in some instances in order to obtain suitable photographs. Photographs are courtesy of the American Iron and Steel Institute, Kaiser Aluminum, LTV Steel, National Steel, The Budd Company.
Standard

Categorization and Properties of Dent Resistant, High Strength, and Ultra High Strength Automotive Sheet Steel

2017-03-22
J2340_201703
This SAE Recommended Practice defines and establishes mechanical property ranges for seven grades of continuously cast high strength automotive sheet steels that can be formed, welded, assembled, and painted in automotive manufacturing processes. The grade of steel specified for an identified part should be based on part requirements (configuration and strength) as well as formability. Material selection should also take into consideration the amount of strain induced by forming and the impact strain has on the strength achieved in the finished part. These steels can be specified as hot-rolled sheet, cold-reduced sheet, uncoated, or coated by hot dipping, electroplating, or vapor deposition of zinc, aluminum, and organic compounds normally applied by coil coating. The grades and strength levels are achieved through chemical composition and special processing. Not all combinations of strength and coating types may be commercially available. Consult your steel supplier for details.
Standard

Chemical Compositions of SAE Alloy Steels

2009-01-27
J404_200901
In 1941, the SAE Iron and Steel Division in collaboration with the American Iron and Steel Institute (AISI) made a major change in the method of expressing composition ranges for the SAE steels. The plan, as now applied, is based in general on narrower ladle analysis ranges plus certain product (check) analysis allowances on individual samples, in place of the fixed ranges and limits without tolerances formerly provided for carbon and other elements in SAE steels (reference SAE J408). ISTC Division 1 has developed a procedure which allows for the maintenance of the grade list in this SAE Standard. This will involve conducting an industry-wide survey to solicit input. This survey will be conducted at a frequency deemed necessary by the technical committee. Criteria have been established for the addition to or deletion of grades from the grade table.
Standard

Former SAE Standard and Former SAE Ex-Steels

2008-12-02
J1249_200812
This SAE Information Report provides a list of those SAE steels which, because of decreased usage, have been deleted from the standard SAE Handbook listings. Included are alloy steels from SAE J778 deleted since 1936, carbon steels from SAE J118 deleted since 1952, and all EX-steels deleted from SAE J1081. Information concerning SAE steels prior to these dates may be obtained from the SAE office on request. With the issuance of this report, SAE J778, Formerly Standard SAE Alloy Steels, and SAE J118, Formerly Standard SAE Carbon Steels, will be retired since they are now combined in SAE J1249. In the future, new assignments to SAE J1081, Chemical Compositions of SAE Experimental Steels, will be given “PS” (Potential Standard) numbers rather than “EX” numbers. The steels listed in Tables 1 and 2 are no longer considered as standard steels. Producers should be contacted concerning availability.
Standard

GENERAL CHARACTERISTICS AND HEAT TREATMENTS OF STEELS

1995-10-01
J412_199510
The information and data contained in this SAE Information Report are intended as a guide in the selection of steel types and grades for various purposes. Consideration of the individual types of steel is preceded by a discussion of the factors affecting steel properties and characteristics. SAE steels are generally purchased on the basis of chemical composition requirements (SAE J403, J404, and J405). High-strength, low alloy (HSLA) steels (SAE J1392 and J1442) are generally purchased on the basis of mechanical properties; different chemical compositions are used to achieve the specified mechanical properties. Because these steels are characterized by their special mechanical properties obtained in the as-rolled condition, they are not intended for any heat treatment by the purchaser either before, during, or after fabrication. In many instances, as in the case of steels listed in SAE J1268 and J1868, hardenability is also a specification requirement.
Standard

INFRARED TESTING

1991-02-01
J359_199102
The scope of this SAE Information Report is to provide general information relative to the nature and use of infrared techniques for nondestructive testing. The document is not intended to provide detailed technical information, but will serve as an introduction to the theory and capabilities of infrared testing and as a guide to more extensive references.
Standard

Infrared Testing

2018-01-09
J359_201801
The scope of this SAE Information Report is to provide general information relative to the nature and use of infrared techniques for nondestructive testing. The document is not intended to provide detailed technical information, but will serve as an introduction to the theory and capabilities of infrared testing and as a guide to more extensive references.