Browse Standards AMS5354F
Historical REVISED 2012-12-20

Steel, Corrosion and Heat Resistant, Investment Castings 13Cr - 2.0Ni - 3.0W Hardened and Tempered to 32 – 38 HRC AMS5354F

This specification covers a corrosion and moderate heat resistant steel in the form of investment castings.
AMS5354G
2023-11-03
Latest
Reaffirmed
AMS5354F
2012-12-20
Historical
Revised
AMS5354E
2006-04-18
Historical
Reaffirmed
AMS5354D
1995-05-01
Historical
Reaffirmed
AMS5354C
1975-06-01
Historical
Revised
AMS5354B
1962-06-01
Historical
Revised
AMS5354A
1959-01-01
Historical
Revised
AMS5354
1947-12-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion and Heat Resistant, Investment Castings 13Cr - 2.0Ni - 3.0W Hardened and Tempered to 32 - 38 HRC

AMS5354G

View Details

STANDARD

Steel, Corrosion-Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb (Nb) - 2.8Cu Solution and Precipitation Heat Treated (H925) 180 ksi (1241 MPa) Tensile Strength (15-5)

AMS5346D

View Details

STANDARD

Steel, Corrosion-Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb (Nb) - 2.8Cu Solution and Precipitation Heat Treated (H1000) 150 ksi (1034 MPa) Tensile Strength (15-5)

AMS5347C

View Details